Annealer door seals

I'm wondering what are some of the ways the group has found to seal annealer doors? I am referring to 2 door front loading annealers. More specifically sealing up the gap between where the two doors meet, not the hinge side of the door.
I usually just create a narrow soft brick wall that the doors can close against to seal the door gap. (Saw this in a Hub annealer originally) It works fine but does impead on getting larger pieces into the oven sometimes.

Wondering what others do?
Reply With Quote
  #2  
Old 06-19-2019, 02:14 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 213
Shawn Everette is on a distinguished road
There is a refractory rope that usually acts as pretty good flexible overlapping seal between the doors. Without knowing more about the door construction it's hard to say if that would work for you. Those middle beams really get in the way sometimes.

Basically this, but I'd prefer a larger diameter.
Reply With Quote
  #3  
Old 06-19-2019, 02:48 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,084
Pete VanderLaan is on a distinguished road
If the doors are yet to be constructed, make one of the doors with a lip on it, fashioned in such a way that the second door can close onto that lip. Seal that with fiberglass woven rope. This way, when the secpnd door is opened, nothing is blocking the center. If you need that space, pop door number one open and the closure will move out of the way.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 06-19-2019, 03:10 PM
David Patchen's Avatar
David Patchen David Patchen is offline
Registered User
 
Join Date: Sep 2005
Location: San Francisco, CA
Posts: 1,877
David Patchen is on a distinguished road
Google 'tadpole gasket'. They are similar to fiberglass rope, except that they have an extra piece of fabric that's easy to pin versus trying to get pins through the rope. It's what the major equipment manufacturers use. I don't know the exact one, but that's the type.
Reply With Quote
  #5  
Old 06-19-2019, 05:41 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,506
Eben Horton is on a distinguished road
Quote:
Originally Posted by David Patchen View Post
Google 'tadpole gasket'. They are similar to fiberglass rope, except that they have an extra piece of fabric that's easy to pin versus trying to get pins through the rope. It's what the major equipment manufacturers use. I don't know the exact one, but that's the type.
Thatís what I would use as well
__________________
<eben epoiese>
Reply With Quote
  #6  
Old 06-19-2019, 11:28 PM
Eric Trulson Eric Trulson is offline
Young Turk
 
Join Date: Sep 2014
Location: Boston
Posts: 104
Eric Trulson is on a distinguished road
https://www.mcmaster.com/8815k32 <--- That's tadpole gasket. I just picked an arbitrary size, although it's in the right ballpark of what I'd use for an annealer door.

Note that the temperature range of the fiberglass ones top out around 1000F, so I would only use them for annealing ovens. For a fusing or casting oven, bump up to the silica fiber/inconel mesh tadpole gaskets.
Reply With Quote
  #7  
Old 06-20-2019, 05:36 AM
Philip Yamron Philip Yamron is offline
Registered User
 
Join Date: Jul 2012
Location: Ann Arbor, MI
Posts: 76
Philip Yamron is on a distinguished road
Thanks everyone!
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 03:23 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.