Spherical Grinding wheel

I'm in need of a few spherical grinding wheels 6" x 220 diamond grit and will possibly be ordering them from China. These are the nickel plated ones. They price out at $65 per. The minimum order is 5. I do not need 5. I would need only 3. Is anyone interested in 2 wheels plus postage from Ohio?
Reply With Quote
  #2  
Old 09-28-2020, 07:16 PM
Brian Graham's Avatar
Brian Graham Brian Graham is offline
Registered Abuser
 
Join Date: Mar 2004
Location: Akron - Ohio
Posts: 549
Brian Graham is on a distinguished road
What is the wheel width and arbor size?
__________________
The revolution will not be televised.
Reply With Quote
  #3  
Old 09-28-2020, 10:04 PM
Marty Kremer Marty Kremer is offline
Registered User
 
Join Date: May 2004
Location: North Yarmouth ME
Posts: 526
Marty Kremer is on a distinguished road
What Brian said-
I might be interested.
Reply With Quote
  #4  
Old 09-29-2020, 12:05 AM
Rick Wilton Rick Wilton is online now
Registered User
 
Join Date: Oct 2005
Location: Calgary, Alberta Canada
Posts: 224
Rick Wilton is on a distinguished road
Have you looked at these ones. You can order 1, I've ordered a bunch of things from these guys are am impressed with the quality for the price. No they aren't the best of the best but are decent... In my opinion https://www.thk.hk/online-cart-dtl.p...ssid=23&id=641
Reply With Quote
  #5  
Old 09-29-2020, 11:37 AM
Henry Halem Henry Halem is offline
Registered User
 
Join Date: Apr 2002
Location: Kent, OH
Posts: 1,435
Henry Halem is on a distinguished road
Quote:
Originally Posted by Rick Wilton View Post
Have you looked at these ones. You can order 1, I've ordered a bunch of things from these guys are am impressed with the quality for the price. No they aren't the best of the best but are decent... In my opinion https://www.thk.hk/online-cart-dtl.p...ssid=23&id=641
Rick, their price is right but all they show is a flat faced wheel. I'm in need of a spherical wheel.
Reply With Quote
  #6  
Old 09-29-2020, 06:48 AM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 1,023
Sky Campbell is on a distinguished road
Henry I bought a set of the 4” and polishing wheels the last time you ordered and was very happy with the quality. Do you know if they have a 4” that is 1” wide as opposed to the 1.5” width of the ones we bought?

The 4” spherical wheels were 1 1/2” wide and a arbor size hole of 1” with many adapter bushings for any size smaller.
Reply With Quote
  #7  
Old 09-29-2020, 12:24 PM
Henry Halem Henry Halem is offline
Registered User
 
Join Date: Apr 2002
Location: Kent, OH
Posts: 1,435
Henry Halem is on a distinguished road
[quote=Sky Campbell;148942]Henry I bought a set of the 4” and polishing wheels the last time you ordered and was very happy with the quality. Do you know if they have a 4” that is 1” wide as opposed to the 1.5” width of the ones we bought?

The link posted by Rick takes you to a company out of Hong Kong that sells the wheels in the 1" width but it seems only in a 6" diameter. It also does not look like they sell a spherical profile as they only show a flat face. I have written to them asking if they sell the spherical profile. Will get back when and if I hear from them.
Reply With Quote
  #8  
Old 09-30-2020, 12:02 PM
David Patchen's Avatar
David Patchen David Patchen is offline
Registered User
 
Join Date: Sep 2005
Location: San Francisco, CA
Posts: 1,912
David Patchen is on a distinguished road
[quote=Henry Halem;148947]
Quote:
Originally Posted by Sky Campbell View Post
Henry I bought a set of the 4” and polishing wheels the last time you ordered and was very happy with the quality. Do you know if they have a 4” that is 1” wide as opposed to the 1.5” width of the ones we bought?

The link posted by Rick takes you to a company out of Hong Kong that sells the wheels in the 1" width but it seems only in a 6" diameter. It also does not look like they sell a spherical profile as they only show a flat face. I have written to them asking if they sell the spherical profile. Will get back when and if I hear from them.
Did you check Kingsley North? They often have good deals on all grinding stuff and you wouldn't have to wait on an import.
Reply With Quote
  #9  
Old 09-30-2020, 05:24 PM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 1,023
Sky Campbell is on a distinguished road
[quote=David Patchen;148970]
Quote:
Originally Posted by Henry Halem View Post

Did you check Kingsley North? They often have good deals on all grinding stuff and you wouldn't have to wait on an import.
I have and they only have a 6” wheels 1 1/2” wide for twice the price of waiting on the boat from overseas.
Reply With Quote
  #10  
Old 09-29-2020, 11:39 AM
Henry Halem Henry Halem is offline
Registered User
 
Join Date: Apr 2002
Location: Kent, OH
Posts: 1,435
Henry Halem is on a distinguished road
Quote:
Originally Posted by Brian Graham View Post
What is the wheel width and arbor size?
6" diameter and 1 inch arbor. Comes with step down arbor plugs to fit most standard machines.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 09:26 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.