No boring mill here. We'll see what happens with flipping them over and drilling from both ends
Reply With Quote
  #202  
Old 04-14-2011, 04:10 PM
Lawrence Ruskin Lawrence Ruskin is offline
Registered User
 
Join Date: Sep 2006
Location: Lions Bay B.C.
Posts: 706
Lawrence Ruskin is on a distinguished road
Got them, and they were very well packed.

All elements intact even though fed ex put a nice ding in the side of the box.

Thanks

....L
__________________
Do or do not....There is no try.

Yoda
Reply With Quote
  #203  
Old 04-14-2011, 05:30 PM
Lawrence Duckworth Lawrence Duckworth is offline
Registered User
 
Join Date: Mar 2010
Location: Gainesville, GA
Posts: 680
Lawrence Duckworth is on a distinguished road
.............

Last edited by Lawrence Duckworth; 03-03-2014 at 06:41 AM.
Reply With Quote
  #204  
Old 04-14-2011, 05:51 PM
John Riepma John Riepma is offline
Registered User
 
Join Date: Apr 2003
Location: Grand Haven, MI
Posts: 516
John Riepma is on a distinguished road
I see you made your own boring mill Lawrence. It takes a determined guy to lay the head all the way over on a Bridgeport. Actually it's easy to get it down, a large pain in the ass to get it back up. Did you use the table feed to drill them or didn't you have a long enough drill?
Reply With Quote
  #205  
Old 04-14-2011, 08:21 PM
Lawrence Duckworth Lawrence Duckworth is offline
Registered User
 
Join Date: Mar 2010
Location: Gainesville, GA
Posts: 680
Lawrence Duckworth is on a distinguished road
Both, all the spindle and the rest of the way with the table….power feed would’ve been nice. Everything fit good so it was worth the pain to set up.
Reply With Quote
  #206  
Old 04-15-2011, 08:00 AM
Lawrence Duckworth Lawrence Duckworth is offline
Registered User
 
Join Date: Mar 2010
Location: Gainesville, GA
Posts: 680
Lawrence Duckworth is on a distinguished road
How's that dip stuff working out for you guys when changing pots and mollys? Is the stuff just to keep the insulation in place and If so what woild you folks think of using something like a fire blanket instead.
Reply With Quote
  #207  
Old 04-15-2011, 09:06 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,280
Pete VanderLaan is on a distinguished road
Jeez, we just used a 5/8th spade bit with an extension on a drill press.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #208  
Old 04-15-2011, 02:32 PM
Lawrence Duckworth Lawrence Duckworth is offline
Registered User
 
Join Date: Mar 2010
Location: Gainesville, GA
Posts: 680
Lawrence Duckworth is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
Jeez, we just used a 5/8th spade bit with an extension on a drill press.
3.875 over! How do you live with yourself...
Reply With Quote
  #209  
Old 04-15-2011, 03:20 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,280
Pete VanderLaan is on a distinguished road
Well, I've learned from bitter experience that the elements are really easy to break, your math not withstanding and that IFB expand when heated ...
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #210  
Old 04-16-2011, 08:05 AM
Lawrence Duckworth Lawrence Duckworth is offline
Registered User
 
Join Date: Mar 2010
Location: Gainesville, GA
Posts: 680
Lawrence Duckworth is on a distinguished road
..so the math is good until ya flip the switch.

Are there any recommended torque specs for the support clamps and strap connections to the mollys. I’m worried they can be over tightened and crush the tubes.
Reply With Quote
  #211  
Old 04-16-2011, 11:37 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,280
Pete VanderLaan is on a distinguished road
I will look in the super Kanthal Handbook but I don't recall any. Make them good and snug if that helps. Once the thing has been turned on and run for two days, go back and tighten everything again. Use the Noalox but never on the elements.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #212  
Old 04-16-2011, 02:53 PM
Jordan Kube Jordan Kube is online now
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,717
Jordan Kube is on a distinguished road
The elements aren't hollow Lawrence. Don't worry about crushing them.

As far as having an element made up I guess it's a personal choice. It's one less thing I have to deal with when an element goes out. It's what I recommend to people when I do installations. Why waste fifteen minutes doing it when you can do it in five? It's also a bad time to have to hunt around for stuff, clear some space, etc. You know you've got one ready to go. The blowing session doesn't have to be totally lost.
__________________
WWUD? Think for yourself.
Reply With Quote
  #213  
Old 04-16-2011, 03:58 PM
Rollin Karg Rollin Karg is offline
Registered User
 
Join Date: Apr 2002
Location: Kechi, KS
Posts: 924
Rollin Karg is on a distinguished road
I in the corner of having one ready to go and all the tools necessary in one place. Just in case it breaks at an inopportune time. Let's make it as easy as possible.
Reply With Quote
  #214  
Old 04-17-2011, 08:15 PM
Lawrence Duckworth Lawrence Duckworth is offline
Registered User
 
Join Date: Mar 2010
Location: Gainesville, GA
Posts: 680
Lawrence Duckworth is on a distinguished road
Ready for dip stuff and straps.

Last edited by Lawrence Duckworth; 03-03-2014 at 06:41 AM.
Reply With Quote
  #215  
Old 04-18-2011, 01:08 AM
Jordan Kube Jordan Kube is online now
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,717
Jordan Kube is on a distinguished road
Forgive me for asking but how do you plan on getting those elements out? They look like they're completely fraxed over. I wouldn't cover any metal parts.
__________________
WWUD? Think for yourself.
Reply With Quote
  #216  
Old 04-18-2011, 06:12 AM
Doug Sheridan
Guest
 
Posts: n/a
I agree with Jordon. Did you cut the frax out from around the top of the brick? The element would get too hot covered like that.
Reply With Quote
  #217  
Old 04-18-2011, 08:19 AM
Lawrence Duckworth Lawrence Duckworth is offline
Registered User
 
Join Date: Mar 2010
Location: Gainesville, GA
Posts: 680
Lawrence Duckworth is on a distinguished road
There is one inch of insulation covering the ceramic/metal clamps. In the duckbill photos I have it appears to me to be covered in dip also... Its not a problem to cut the insulation out of the way if you guys think leaving them covered is a disadvantage.
Reply With Quote
  #218  
Old 04-18-2011, 09:31 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,280
Pete VanderLaan is on a distinguished road
It is a problem. If you leave them covered they will fail very quickly - possibly in less than two weeks if you run hot at all. The clamps and the straps need to be completely exposed and air cooled if you want any life from them at all. What you are doing is great for my boat payment plan, but it offers no other benefit at all. Steve and Brent built air cooling manifold which help keep the straps cool. I would strongly suggest you do the same.

Don't ever try to cover up metal with insulation in a furnace. It usually takes just a few days for it to vaporize.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #219  
Old 04-18-2011, 11:40 AM
Tom Bloyd Tom Bloyd is offline
Registered User
 
Join Date: Nov 2007
Location: Kansas city
Posts: 145
Tom Bloyd is on a distinguished road
Rollin Karg posted a air cooled manifold awhile back. Look in the archives it looked pretty nice.
Reply With Quote
  #220  
Old 04-18-2011, 12:58 PM
Lawrence Duckworth Lawrence Duckworth is offline
Registered User
 
Join Date: Mar 2010
Location: Gainesville, GA
Posts: 680
Lawrence Duckworth is on a distinguished road
See what you guys think of this.

Tom, i'll look at tat tonight...thanks. (just now learning to type with my thumbs)

Last edited by Lawrence Duckworth; 03-03-2014 at 06:41 AM.
Reply With Quote
  #221  
Old 04-18-2011, 04:01 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,280
Pete VanderLaan is on a distinguished road
That seems fine to me.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #222  
Old 04-18-2011, 07:36 PM
Tom Bloyd Tom Bloyd is offline
Registered User
 
Join Date: Nov 2007
Location: Kansas city
Posts: 145
Tom Bloyd is on a distinguished road
Lawrence, it"s under the thread "moly cooling". If I wasn't such a ludite I would link you to it,but.......
Reply With Quote
  #223  
Old 04-18-2011, 08:57 PM
Lawrence Duckworth Lawrence Duckworth is offline
Registered User
 
Join Date: Mar 2010
Location: Gainesville, GA
Posts: 680
Lawrence Duckworth is on a distinguished road
Quote:
Originally Posted by Tom Bloyd View Post
Lawrence, it"s under the thread "moly cooling". If I wasn't such a ludite I would link you to it,but.......
Thanks Tom, I found it. Good discussion and information, great photo of the strap connections too.



Transformer showed up today........could get ugly
Reply With Quote
  #224  
Old 04-19-2011, 05:03 AM
Hugh Jenkins Hugh Jenkins is offline
Registered User
 
Join Date: Sep 2006
Location: Honoka'a, HI
Posts: 1,010
Hugh Jenkins is on a distinguished road
I have to agree, electric gets ugly really quickly!!!
__________________
Aloha, Hugh
Reply With Quote
  #225  
Old 04-19-2011, 10:03 AM
Lawrence Duckworth Lawrence Duckworth is offline
Registered User
 
Join Date: Mar 2010
Location: Gainesville, GA
Posts: 680
Lawrence Duckworth is on a distinguished road
Actually....electrical work is simple. It either works or it doesnt.

Last edited by Lawrence Duckworth; 04-19-2011 at 10:05 AM. Reason: spelling
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 07:23 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.