Cooling the studio

Anyone got one of these. Is it a scam?
Franklin
Attached Images
File Type: jpg C4693F0B-7597-4944-9C42-FE8DA649A3FC.jpg (40.8 KB, 44 views)
Reply With Quote
  #2  
Old 08-14-2020, 09:07 AM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 694
Shawn Everette is on a distinguished road
Yes, yes that looks like a scam. Consider the size of a window unit and how that won't cool much more than a room.

Big evap coolers are the way to go, if you have the right climate, but I'm afraid that we are sol.
Reply With Quote
  #3  
Old 08-14-2020, 09:15 AM
Rich Samuel's Avatar
Rich Samuel Rich Samuel is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle, WA
Posts: 2,555
Rich Samuel is on a distinguished road
It's a mini swamp cooler, and won't cool a room. (You'd be lucky if it cooled your face!) Caveat Emptor.

https://www.youtube.com/watch?v=GQdtfRHJTHQ
Reply With Quote
  #4  
Old 08-14-2020, 09:19 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,171
Pete VanderLaan is on a distinguished road
https://www.scamdoc.com/view/335034

It's an evaporative cooler Franklin, a very small one. Try sweating in front of a fan instead.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 08-14-2020, 09:32 AM
Steven O'Day Steven O'Day is online now
Registered User
 
Join Date: Jun 2002
Location: portland oregon
Posts: 336
Steven O'Day is on a distinguished road
I tried an evaporative cooler in my studio in Santa Fe. Basically a greenhouse size mat covering the garage door and a huge blower. It worked great if you were standing in front of it but at the work station it was worse than nothing. The humid air would heat up and not only was it hot it no longer was a dry heat!
Reply With Quote
  #6  
Old 08-14-2020, 10:35 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,046
Franklin Sankar is on a distinguished road
Interesting, How they get away with these scams
Franklin
Reply With Quote
  #7  
Old 08-14-2020, 11:16 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,171
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Steven O'Day View Post
I tried an evaporative cooler in my studio in Santa Fe. Basically a greenhouse size mat covering the garage door and a huge blower. It worked great if you were standing in front of it but at the work station it was worse than nothing. The humid air would heat up and not only was it hot it no longer was a dry heat!
****
Way back when GAS was held at Philabaum's studio in Tucson, they had a huge Evaporative cooler over the marver. Lino made them turn it off when he demonstrated.

Franklin, fraud in AMERICA is as popular as Apple Pie.

Steve, did you get my PM?
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #8  
Old 08-14-2020, 12:00 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,046
Franklin Sankar is on a distinguished road
Thanks for the site. It is great.what is happening to the great America. Sad
Franklin
Reply With Quote
  #9  
Old 08-14-2020, 12:24 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 694
Shawn Everette is on a distinguished road
Quote:
Originally Posted by Franklin Sankar View Post
what is happening to the great America. Sad
Franklin
There went my belly laugh for the day.
Reply With Quote
  #10  
Old 08-14-2020, 01:59 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,171
Pete VanderLaan is on a distinguished road
Land of the big bellied undereducated biker.

The single best way to have a cool studio is to insulate your well ventilated hood and to keep the tooling under the hood. What's a tool you might ask?
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #11  
Old 08-14-2020, 05:30 PM
Larry Cazes Larry Cazes is offline
Registered User
 
Join Date: Feb 2006
Location: San Jose, CA
Posts: 1,026
Larry Cazes is on a distinguished road
Quote:
Originally Posted by Franklin Sankar View Post
Thanks for the site. It is great.what is happening to the great America. Sad
Franklin
These come from China actually. You think thats scammy just check out the crap our media pushes. All of them. In just the right climate swamp chillers are very effective but most good ones are the size of a full HVAC unit. These are laughable.
Reply With Quote
  #12  
Old 08-14-2020, 05:56 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,171
Pete VanderLaan is on a distinguished road
Hey! The armpit size one is special.!!
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #13  
Old 08-17-2020, 11:25 AM
Mark Rosenbaum's Avatar
Mark Rosenbaum Mark Rosenbaum is offline
Registered User
 
Join Date: Apr 2002
Location: New Orleans, LA
Posts: 1,082
Mark Rosenbaum is on a distinguished road
I have a large industrial -sized one if anyone is interested....
Reply With Quote
  #14  
Old 08-17-2020, 01:45 PM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 704
Art Freas is on a distinguished road
These are nice for breaks, uses standard Ryobi 18V batteries. You don't need a hose will just sit on top of a drywall bucket.


https://www.homedepot.com/p/RYOBI-18...F01B/313313435
Reply With Quote
  #15  
Old 08-17-2020, 01:56 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,171
Pete VanderLaan is on a distinguished road
If it was hot, I actually just soaked my Tilley Hat in a big tub of water, put it on and let it trickle down. Very low tech and I loved it. It would be ready to resoak by the next piece.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #16  
Old 08-17-2020, 02:03 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 694
Shawn Everette is on a distinguished road
I moved to the articulating floor driers several years ago. High volume of air moved, but easy to aim it to keep it off your piece.
Reply With Quote
  #17  
Old 08-17-2020, 03:44 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
Registered User
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,239
Greg Vriethoff is on a distinguished road
Best thing I have found (and it's low-tech!) is a wet cloth or bandana wrapped around the back of my neck. There are commercially produced versions that have a chill pack or are made of microfiber. I don't think it's so much about how cold the moisture is, but the evaporation. Drink plenty of fluids (room temp. water), and circulate the air. Of course I don't have to tell you about circulation since we all have properly ventilated shops.

Here's a commercial one. I've only ever used washcloths, so I don't know what works better. I know you don't have REI Franklin, but I like them better than the other evil corporations.

https://www.rei.com/product/691097/k...0073&store=115
Reply With Quote
  #18  
Old 08-17-2020, 11:46 PM
Scott Dunahee's Avatar
Scott Dunahee Scott Dunahee is offline
Registered User
 
Join Date: Apr 2002
Location: Madison, WI
Posts: 642
Scott Dunahee is on a distinguished road
I still say put your propane tank in a tub of water, recirc that through a copper coil mounted to the face of a fan. Propane gassing off is cold, making the water cold, making the water pumped through the "radiator" coil cold... free cold air blowing on you?

Never tried it but I think it should work....

BSD
__________________
That's all right. I never expected there to be a blue light special on enlightenment...
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 01:57 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.