Safe, but inexpensive way to store corrosives?

I'm trying to organize one of the many storage areas in my shop and realized that the two bottles of acids that I have for making aqua regia, which I have stored there in their original cardboard shipping boxes for 2 years since I last used some, have started to oxidize the painted metal shelf they're sitting on. I suppose enough fumes are getting out to do be able to do that. I looked up corrosive storage cabinets, but even the small ones are larger than I need and the prices seem insane. Can I just put these bottles, making sure they stay upright, in a plastic bucket with a lid and a skull-and-crossbones drawn on the side? And would it need any tiny bit of ventilation or no? Thanks in advance.
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #2  
Old 09-10-2020, 06:43 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,114
Pete VanderLaan is on a distinguished road
In the fire dept, we always packed our materials like this in silica . It lowered the temp and stopped the action.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 09-10-2020, 09:23 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 667
Shawn Everette is on a distinguished road
Plastic should be polyethylne for most acid. If it's not got a way to vent, it will find one.... hopefully not in your face.
Reply With Quote
  #4  
Old 09-11-2020, 11:39 AM
Josh Bernbaum Josh Bernbaum is offline
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 711
Josh Bernbaum is on a distinguished road
So a polyethylene container with silica at the bottom and a couple small vent holes in the lid?
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #5  
Old 09-11-2020, 12:49 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,114
Pete VanderLaan is on a distinguished road
Indeed. I think you can find lidded containers at Amazon at the least. You know where to get the silica. I was always impressed when we did haz mat stuff in Santa Fe how effective the silica was. Sometimes it took other approaches- sulfuric acid spills and we would make gypsum using calcium carbonate. Having the labs up on the hill and having the big trucks of acids coming through on the interstate every monday morning at 3;00 am kept us tuned in. That, giant containers of liquid oxygen, always mondays. Mayberry it wasn't. The only sustained incident was closing the interstate a few times for gas trucks overturning and contaminating the shit out of everything. That we had to excavate for what seemed like forever.

What is disconcerting to me here is how cans rust out. I have stuff that would never have changed in NM but here? aerosols seem the worst and that includes insecticides, paint cans, really corrosive.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #6  
Old 09-11-2020, 04:59 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,759
Eben Horton is on a distinguished road
Keep it in the left side of the fridge. Food on the right.
__________________
<eben epoiese>
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 11:30 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.