Does anyone have any experience tempering COE96 glass rondels for an outdoor art installation?
Reply With Quote
  #2  
Old 05-24-2017, 06:14 PM
Mike McCain
Guest
 
Posts: n/a
Break out the Salt Peter

https://en.m.wikipedia.org/wiki/Chem...ngthened_glass
Reply With Quote
  #3  
Old 05-24-2017, 07:32 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,932
Pete VanderLaan is on a distinguished road
and then try to avoid getting on a DHS watch list for buying it.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 05-24-2017, 07:37 PM
Tom Fuhrman Tom Fuhrman is offline
Registered User
 
Join Date: Apr 2002
Location: hills of Tennessee
Posts: 1,443
Tom Fuhrman is on a distinguished road
check with John Lewis, he's done lots of outdoor installations. I suspect that may have been a spec for some installation written by an architect that has no idea what the nature of handblown glass is really all about. The outdoor installations I've done were never tempered and have been outside for going on 20 years. If safety is an issue then you may have them coated with some of the clear silicone material that keeps them from breaking into slivers but usually makes the glass look terrible with no luster to it.
Reply With Quote
  #5  
Old 05-26-2017, 09:43 AM
Rick Wilton Rick Wilton is online now
Registered User
 
Join Date: Oct 2005
Location: Calgary, Alberta Canada
Posts: 220
Rick Wilton is on a distinguished road
Good luck, I worked at a glass plant for a while and we tried tempering spectrum sheet glass, bullseye and even float glass that had been fused together. The results were always the same they'd explode into millions of pieces, some would die immediately during the quench others would tease you and survive to at least get out of the tempering furnace. All it takes is an airbubble, a seed, a speck of refractory etc for it to explode. Even perfectly clear float glass has a failure rate for the same reasons. When I worked there we made a few outdoor installations using sheets of spectrum for a huge outdoor monument. These sheets were laminated to tempered glass to make them meet code.

Chemical tempering does make the glass stronger but it does NOT meet the same code guidelines as heat tempering. Chemical tempered glass still breaks like regular glass.... ie sharp
Reply With Quote
  #6  
Old 05-26-2017, 12:37 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,932
Pete VanderLaan is on a distinguished road
I think one of the real troubles with installation type jobs is the place that wants it gets lawyers and bureaucrats too close to the process. They all live to indemnify themselves. In Public Installations, you wind up filling out tons of forms on your hiring practices, compliance with codes, on and on. In bathrooms, it's a total nightmare. I can't really get excited about having to jump through someone's hoops over trying to get that work and this sounds a lot like those hoops.

As Edward Abbey once said "I smell Lawyers here..."
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #7  
Old 05-26-2017, 02:23 PM
Tony Serviente Tony Serviente is offline
Registered User
 
Join Date: Mar 2005
Location: Ithaca, NY
Posts: 155
Tony Serviente is on a distinguished road
Bob at His Glassworks used to sell something called FlexTec. It is a thick 2 part epoxy that you brush onto the glass. In case of glass failure it holds the pieces together quite well. I tested it and it was very good. It is the same concept as laminated, but a surface application. It does not leave a clear surface, and its working time is very limited, but it was just what we needed for a lamp job.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 09:18 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.