The Harzkristall Nuggets are COE 100 glass

HUH??? quote from their website "The Harzkristall Nuggets are COE 100 glass. With the latest technology it's possible to melt nuggets in every composition according to the customer's request."

https://www.harzkristall-nuggets.com/
Reply With Quote
  #2  
Old 03-10-2020, 12:10 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,932
Pete VanderLaan is on a distinguished road
I believe Peter Kuchinke is involved with this company and it's the latest in a line of them. The EU largely works around a 97.5 standard and that was where cristalica was when introduced. Kuchinke had also worked with a melt facility in Romania and that relationship stopped. Then he had a very public falling out with the Dobern Group and moved on. He is apparently doing this.

So, 100 L.E.C. certainly won't do anyone much good. It's too low for Lauscha, too high for anyone else. You really have to wonder what the thinking and consulting process is with these people. To assume that they will flip expansions on a dime involves changing formulation which means differing glass in the furnace. That implies tonnage to do it cleanly. This seems unlikely to the point of risky.

Scott has told me that much of the EU has turned to GLASMA as a batch. Given the cast of characters in the cullet war, not a bad plan.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 03-10-2020, 02:40 PM
John Croucher's Avatar
John Croucher John Croucher is offline
Registered User
 
Join Date: Jul 2003
Posts: 61
John Croucher is on a distinguished road
Cristalica nuggets were sold as a measured LEC 100 x 10-7 20-300oC glass. +/-2 points. Presumably the new Harzkristall nuggets are a similar formulation. I wouldn't place too much emphasis on the exact dilatometric number. Viscosity is also important. At the end of the day Cristalica was pretty compatible with SP87 and Spectrum Version 2.0 It worked fine with Gaffer.
See Cristalica data sheet: https://cristalica-studioglass.com/Datenblatt/?lang=1
Reply With Quote
  #4  
Old 03-10-2020, 04:53 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,932
Pete VanderLaan is on a distinguished road
My cristalica paperwork indicated a 97.5
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 08:42 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.