Question Copper / gold / brown aventurine

Some one brought us a piece with what looks like a metallic copper colored aventurine frit in the piece. We are not sure if it is a copper or gold or brown aventurine. Does anyone know a manufacturer that does copper aventurine? Thanks much
Reply With Quote
  #2  
Old 02-14-2015, 06:58 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,115
Pete VanderLaan is on a distinguished road
True aventurines are made in pots only and broken up when cooled. The only true aventurines are chrome and copper. Chrome is not that difficult to make but the copper is far more elusive. I don't know of manufacturers of the product although a lot of stuff is being done with a mica now but it's not the real deal.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 02-14-2015, 08:02 AM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 1,021
Sky Campbell is on a distinguished road
I see a lot of that sparking copper color in Chinese imports. They seem to really love it.

I do think most of what I see is mica.
Reply With Quote
  #4  
Old 02-14-2015, 09:23 AM
Kenny Pieper Kenny Pieper is offline
Registered User
 
Join Date: Feb 2003
Location: Burnsville N.C.
Posts: 844
Kenny Pieper is on a distinguished road
Olympic has aventurine.
Reply With Quote
  #5  
Old 02-14-2015, 09:55 AM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 693
Art Freas is on a distinguished road
Pete, thanks that really explains it this was definitely a copper based aventurine. I have used the chrome based but had not seen the copper before.

Kenny, thanks for the steer to olympic. We have looked at the frit there and they have a gold aventurine that seems close but it looks to be chrome based.
Reply With Quote
  #6  
Old 02-14-2015, 12:06 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
Registered User
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,230
Greg Vriethoff is on a distinguished road
The aventurine at Olympic is made by Reichenbach.

Kugler also makes it, and you can get it here.

I think those are the only two commercially produced gold aventurines that are made for our purposes. I don't have any opinion on which is better, nor can I vouch for how well they fit with whatever else you throw into your glass.

Spectrum produces aventurine in black, blue, and green, but I believe those are chrome. They are tested at 96.
__________________
Temperature and time.
Reply With Quote
  #7  
Old 02-14-2015, 03:18 PM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is offline
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 773
Michael Ahlefeldt-Laurvig is on a distinguished road
Yes, I have both the green and the copper- the green can is marked Riechenbach, but the other is only marked as copper. These are maybe 10 years old so it may not be up to date.
Reply With Quote
  #8  
Old 02-16-2015, 02:20 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,115
Pete VanderLaan is on a distinguished road
Until someone can definitively prove to me those other colors are true aventurines, I'm sticking to my story that chrome and copper as the only true aventurines and keep in mind they are going to be pretty cordy and if blown out too thin, pretty ugly. To reitierate for those of you that don't know the process, the glass is melted in a pot and then the pot is shut down and cooled. The crystals form between 1700 and probably 1400F in the pot. The pot is then taken from the furnace and broken. The glass is salvaged as chunks, not rod. You aren't going to get any rod. Being a pot vendor, I do like the part about breaking the pot. Pure goosbumps.

One of the things that has struck me in color making is that you would think you could take something like a chrome aventurine green and add cobalt and get a different color, or to do similar things to the copper stuff. Invariably, the addition of that saturation colorant really messes with the crystal forming capacity of the pot glass itself. I have found that in trying to Make Mark Peiser's high density opaque titanium alumina magnesium silicate. If left alone, it is the single densest glass I have ever seen in my life and Scott Benefield and I were able to slightly adjust the expansion of it to where it fit a 96 but it is hopelessly unreliable when you do try to do that as Mark acidly points out in his paper on that subject which I read and reread. We just nudge the expansion, just nudge and it goes amber transparent and then blows out the pot.This glass is 11 percent alumina! I really want this glass since it has such enormous potential in the filigrana trade. Good luck making it, and good luck making the faux aventurines as true ones. Glass remembers everything you ever do to it. Keep in mind that there are vendors everywhere and even more in Seattle that will tell you what you want to hear.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #9  
Old 02-16-2015, 05:51 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
Registered User
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,230
Greg Vriethoff is on a distinguished road
FWIW, the gold and the blue are only available in chunk.
__________________
Temperature and time.
Reply With Quote
  #10  
Old 02-16-2015, 06:18 PM
Tom Fuhrman Tom Fuhrman is offline
Registered User
 
Join Date: Apr 2002
Location: Lakeland, Florida
Posts: 1,463
Tom Fuhrman is on a distinguished road
the Italians have been making both for a long time. I don't know of any of them that sell and market it for use other than their own. I have a feeling if it is used with high expansion lead glasses there is a better chance of getting it to fit and remain intact.
Reply With Quote
  #11  
Old 02-18-2015, 10:35 AM
Dave Bross Dave Bross is offline
Registered User
 
Join Date: Apr 2002
Location: Archer FL(near Gainesville)
Posts: 2,952
Dave Bross is on a distinguished road
I bought it years ago from jewelry suppliers as the chunks.

Very high lead content. It would "fit" an amazing range of glasses without cracking/exploding from stress due to mismatch.

All the old time formulas for it are VERY heavy on the lead.
__________________
Art is not a thing...it's a way.
Reply With Quote
  #12  
Old 02-18-2015, 11:54 PM
David Hopman David Hopman is offline
Registered User
 
Join Date: Mar 2009
Location: Sutter Creek, CA
Posts: 442
David Hopman is on a distinguished road
I have a kilo of the Kugler gold adventurine #1 frit and a kilo of the Kugler blue adventurine #1 frit. Neither is compatible with any of the batches that I have used.
Reply With Quote
  #13  
Old 02-19-2015, 01:03 PM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is offline
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 773
Michael Ahlefeldt-Laurvig is on a distinguished road
It is compatible with glasma
Reply With Quote
  #14  
Old 02-19-2015, 04:51 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,115
Pete VanderLaan is on a distinguished road
GLASMA what? There are lots of GLASMA's

Chrome is almost always a real refractory problem child and worth avoiding. Copper stuff on the other hand tends in the opposite direction and makes for some very strange runny glasses with bizzare viscosities. I think some people go out of their way to get into difficulties.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #15  
Old 02-19-2015, 11:35 PM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 693
Art Freas is on a distinguished road
Went to see Lino work today. There on the color table taunting me was a 2-3 kilo chunk of gold aventurine.
Reply With Quote
  #16  
Old 02-20-2015, 01:56 AM
David Patchen's Avatar
David Patchen David Patchen is offline
Registered User
 
Join Date: Sep 2005
Location: San Francisco, CA
Posts: 1,912
David Patchen is on a distinguished road
Uroboros sells a green avventurine that's 96 COE/LEC. I've used it successfully with Spruce Pine. But be careful--it's easy to make stuff that looks like a bass boat/1970s motorcycle helmet.
Reply With Quote
  #17  
Old 02-20-2015, 03:31 AM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is offline
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 773
Michael Ahlefeldt-Laurvig is on a distinguished road
Right- I should have said Glasma #33. Ive used large amounts of #5 and 33 and to a lesser extent 22 and 3? and as Ive mentioned before color compatibility has never been an issue for me except with cad reds and yellows. One time an issue with opal white making small things. I only use german colors. Its very seldom discussed over here and if it is then its usually someone having run into a odd batch of color that causes problems, but its extremely rare to hear about and if anything it has gotten more seldom over time. Quality has gotten much better over the years.
I crack off and saw a lot of things and it would show itself immediately if there was strain.
Over the whole of my time blowing Ive only had 2 or 3 pieces come back to me inexplicably broken, and I cant even then point to blaming the color. Ive just written it off as odd things happen or the customer has done a hot- cold wash or something and wont stand up to making a mistake (or not understanding it)
In all honesty- Ive never had the green in production- its very dense/dark color and not at all as sparkly as the copper.

Last edited by Michael Ahlefeldt-Laurvig; 02-20-2015 at 03:57 AM.
Reply With Quote
  #18  
Old 02-20-2015, 12:08 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,115
Pete VanderLaan is on a distinguished road
Most of the German colors contain lead with what I now understand to be a new grouping from Reichenbach not having it. The lead allows for quite a bit of tolerance with viscosity differences when matched to most clears in the 96 range. Cadmium glasses will not color well in the presence of lead ( this is an understatement unless you like shit brown) so they have to be made in zinc potash base glass which doesn't have those tolerances built in. As the EU continues to tighten the noose on toxic chemicals that can reach their landfills, I have to wonder what will finally become of the lead in color rod issues. Waterford simply left Ireland after the lead prohibitions set in for decanters and tableware.

Lead is prohibitively expensive in this country now and production of lead monosilicate has simply ceased. The monosilicate was the only form which you could get on your skin without issues.

I can still get lead in Shanghai and I can make lead glasses there but exporting them is an issue as well. I can't ship the monosilicate to myself without getting an EPA permit and I don't want to jump through that hoop. So, I'll either go make my lead stuff in Shanghai or watch the sun go down on the limited supplies I still have.

Chrome is very refractory stuff and the green aventurine is the easy one to make. I remain firm that Copper aventurine is the only other true aventurine out there.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #19  
Old 02-21-2015, 04:10 PM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 693
Art Freas is on a distinguished road
Pete
Question are there any other theoretical aventurines out there looking at the periodic table?
Reply With Quote
  #20  
Old 02-21-2015, 04:49 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,115
Pete VanderLaan is on a distinguished road
I think based on their positions on the table that silver and gold would be feasible but never were pursued because of the costs of the metals. It takes a lot to make it work and it isn't really reliable.

If someone says it's a gold aventurine, it isn't. Think Copper and chrome and not nearly so much copper. Copper is hard.

Positioning yourself with stuff that no one else can do is really a skills based enterprise and it takes years.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #21  
Old 02-22-2015, 01:17 AM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is offline
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 773
Michael Ahlefeldt-Laurvig is on a distinguished road
Kugler has a wide range of lead free colors also- see menu on the left

http://www.kuglercolors.de/english/default_e.htm
Reply With Quote
  #22  
Old 02-24-2015, 11:45 PM
Rich Samuel's Avatar
Rich Samuel Rich Samuel is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle, WA
Posts: 2,551
Rich Samuel is on a distinguished road
Speaking of green aventurine, this is from last night's "Antiques Roadshow."

(Bonus: Can you spot the appraiser's boo-boo, kids? )

http://www.pbs.org/wgbh/roadshow/archive/201401A31.html

Last edited by Rich Samuel; 02-24-2015 at 11:48 PM.
Reply With Quote
  #23  
Old 02-24-2015, 11:58 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
Registered User
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,230
Greg Vriethoff is on a distinguished road
Quote:
Originally Posted by Rich Samuel View Post
Speaking of green aventurine, this is from last night's "Antiques Roadshow."

(Bonus: Can you spot the appraiser's boo-boo, kids? )

http://www.pbs.org/wgbh/roadshow/archive/201401A31.html
I sat through a bunch of bs about how the 1% is making things better for everybody and didn't see anything relevant to the glass piece in question.
__________________
Temperature and time.
Reply With Quote
  #24  
Old 02-25-2015, 03:37 AM
Rich Samuel's Avatar
Rich Samuel Rich Samuel is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle, WA
Posts: 2,551
Rich Samuel is on a distinguished road
Quote:
Originally Posted by Greg Vriethoff View Post
I sat through a bunch of bs about how the 1% is making things better for everybody and didn't see anything relevant to the glass piece in question.
Huh?
Reply With Quote
  #25  
Old 02-25-2015, 07:09 AM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
Registered User
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,230
Greg Vriethoff is on a distinguished road
Quote:
Originally Posted by Rich Samuel View Post
Huh?
I'm not sure why, but all I got was a commercial when I tried playing the video.
__________________
Temperature and time.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 10:44 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.