Question Blue Sulphur

Weyl, in Coloured Glasses (pg. 257-258), and Volf, in A Chemical Approach to Glass (pg. 538), describe making a pure "ultramarine sulfur blue". They both point out that this is done in "borate melts". So my questions are a)has anyone here ever tried this? And b) Is a "borate melt" a batch that contains borax/boric acid or is this implying that it's only attainable in borosilicates? Im going to be doing some sulphur melts/experiments in the next month and thought I'd give the sulphur blue a try, if anyone has any experience to share, I'm all ears. Thanks!
Reply With Quote
  #2  
Old 08-11-2019, 07:18 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,285
Pete VanderLaan is on a distinguished road
I have never done a melt in sulfur that did not do one of two things.
A: make an Amber
B: Really stink up the joint.

I'll read about it. If it does do what you suggest, it would likely be in a boron based glass but I have never heard of it.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 08-11-2019, 10:58 AM
Paul Stout Paul Stout is offline
Registered User
 
Join Date: Aug 2015
Location: Tucson AZ
Posts: 18
Paul Stout is on a distinguished road
ďThe process for making these glasses is quite simple. Sulphur, or an alkali sulphide, is dissolved in molten borax, and into the brown melt excessive boric oxide or phosphoric oxide is stirred. The color changes at first to dirty yellow, then to Grey and finally into a pure blue. This blue color being due to elementary sulphur cannot be obtained in glasses which contain major amounts of zinc, cadmium, or other ions of heavy metals with a pronounced affinity for sulphur.Ē
-Coloured Glasses, Weyl, pg. 258
Sounds like a fun, if stinky, experiment if nothing else!
Reply With Quote
  #4  
Old 08-11-2019, 02:37 PM
Bradley Howes Bradley Howes is offline
Registered User
 
Join Date: Mar 2015
Location: Alfred University
Posts: 62
Bradley Howes is on a distinguished road
A borate glass, as I understand it, is a single component glass that is made up of B2O3. It melts into a vitreous soup at 450ļC (842ļF). Strangely, it has a coordination of 3, that means for every boron atom, it is bonded to 3 oxygens.
I've used boric acid as a flux to purify some gold. The gold formed a bead at the bottom of the crucible and the glass above it dissolved most everything that wasn't gold. When this glass is poured out of the crucible, it starts off perfectly clear and transparent but within an hour, the surface becomes cloudy because it absorbed water from the air. For any glassblower that primarily uses silica as their glass former, borate glasses aren't compatible in any way.
Reply With Quote
  #5  
Old 08-12-2019, 12:54 PM
Josh Bernbaum Josh Bernbaum is offline
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 728
Josh Bernbaum is on a distinguished road
Copper and cobalt donít smell.
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #6  
Old 08-13-2019, 10:10 AM
Paul Stout Paul Stout is offline
Registered User
 
Join Date: Aug 2015
Location: Tucson AZ
Posts: 18
Paul Stout is on a distinguished road
Thatís true, and I do love copper blues, but Iím going to be using sulfur in the traditional way anyhow, so why not try (in the quest for knowledge and understanding and such). Also supposedly the blue comes from elemental sulfur which doesnít stink, only itís compounds do, so theoretically this sulfur blue wouldnít smell either. But not having done it yet, I donít know. Iíll post results, good, bad or indifferent just in case anyone else is interested.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 02:33 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.