Quote:
Originally Posted by Marc Carmen View Post
Josh, I'm dying to try the durissimo. If it's a similar formula to Nero duro then it's a lead free iron sulfide black. Iron sulfide glass is not only naturally stiff but also incredibly brittle. Old glass container literature mentions that it is a cheap and easy way to black glass, if only it didn't make such an impractically brittle bottle.

Man, I have sooo many bubbly black filigrana in my student work haha.
It's not just stiff, it's CRAZY stiff! Definitely the stiffest glass I've ever played with and makes the white duro feel like enamel. I gather on the new black the instant it stops moving, which is literally walking from the gh to the furnace. If you lose the core heat you're toast. If you don't transfer it directly to a stick you're toast. Gathers needs to be done before the previous one fully sets up. Pulls need to be really hot with a faster walk than usual. If you don't have the black poking out of the end of the setup and quench before you stick to the post, you're toast. It's actually super fun to work with because it's so quirky. I've not had great luck keeping it jet black--I think it might have something to do with our gh running a bit rich (maybe Pete can explain what's up w/this). It's been going graphite grey on me--I'm going a few things to try to avoid this. I've been pulling it into cane, then bundling the cane and making murrine. I haven't used the murrine yet, but it looks excellent.

If you're into twisty cane, definitely try some of this stuff, it's wild and so much fun.

Last edited by David Patchen; 11-03-2017 at 01:17 AM.
Reply With Quote
  #27  
Old 11-03-2017, 09:10 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,491
Pete VanderLaan is on a distinguished road
I have not melted sulfide blacks so I'm not able to comment. Lino ran rosin blacks that were remarkable in themselves. Mine are simply chock full of oxides blotting out any color transmission. I would think Alumina is playing a major role.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #28  
Old 11-03-2017, 10:29 AM
Scott Benefield Scott Benefield is offline
Registered User
 
Join Date: Apr 2002
Location: Ballintoy, Northern Ireland
Posts: 87
Scott Benefield is on a distinguished road
I'd be interested in hearing how it looks when you push the Gaffer durissimo that far, David. Stiff is one thing (as Pete says, alumina will get you that) but if it doesn't stay jet black at a hair's thickness....then what's the point?

Lino's rosin black was all that, but the melts he was doing at the old Manifesto facility were kind of unpredictable. Very fine bubbles would only appear in the final application, but not in the initial cane pull--occasionally. It was impossible to know if you had a good melt until you had taken it that far, but by then you were stuck with whatever you had. Lots of it went into the landfill.
Reply With Quote
  #29  
Old 11-03-2017, 10:46 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,491
Pete VanderLaan is on a distinguished road
In the black that I periodically melt, I do pull the cane out into extremely fine thread and then taking two fingernails and run down the thread. If there's anything in it, including bubbles, you will feel them.
My larger question is really whether the gas is coming back out of solution or whether it's just in the finished rod as trapped gas. There's a difference. Color rod can be overworked.

Making color is actually really hard when you consider the standard you have to achieve . In the final analysis, it should be dense black as Scott says, or what's the point?
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #30  
Old 11-03-2017, 10:46 AM
Kenny Pieper Kenny Pieper is offline
Registered User
 
Join Date: Feb 2003
Location: Burnsville N.C.
Posts: 835
Kenny Pieper is on a distinguished road
Quote:
Originally Posted by Scott Benefield View Post

Lino's rosin black was all that, but the melts he was doing at the old Manifesto facility were kind of unpredictable. Very fine bubbles would only appear in the final application, but not in the initial cane pull--occasionally. It was impossible to know if you had a good melt until you had taken it that far, but by then you were stuck with whatever you had. Lots of it went into the landfill.
I have melted that black a couple of times with no problems. Its crazy how it catches on fire when it gets charged. I stays black that's for sure!
Reply With Quote
  #31  
Old 11-03-2017, 11:57 AM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,572
Eben Horton is on a distinguished road
Quote:
Originally Posted by Kenny Pieper View Post
I have melted that black a couple of times with no problems. Its crazy how it catches on fire when it gets charged. I stays black that's for sure!
Did you ever go back ??
Reply With Quote
  #32  
Old 11-03-2017, 12:55 PM
Kenny Pieper Kenny Pieper is offline
Registered User
 
Join Date: Feb 2003
Location: Burnsville N.C.
Posts: 835
Kenny Pieper is on a distinguished road
Quote:
Originally Posted by Eben Horton View Post
Did you ever go back ??
Back where?
Reply With Quote
  #33  
Old 11-03-2017, 03:50 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,572
Eben Horton is on a distinguished road
Quote:
Originally Posted by Kenny Pieper View Post
Back where?
It’s a joke
Reply With Quote
  #34  
Old 11-03-2017, 04:27 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
rEgisturd Spelunker
 
Join Date: Jan 2007
Location: USSA
Posts: 2,124
Greg Vriethoff is on a distinguished road
Quote:
Originally Posted by Eben Horton View Post
It’s a joke
A rather off-color joke, Eben...

(O)
__________________
I loves Dale gilhooly
Reply With Quote
  #35  
Old 11-03-2017, 05:40 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,491
Pete VanderLaan is on a distinguished road
black humor
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #36  
Old 11-04-2017, 10:10 AM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,572
Eben Horton is on a distinguished road
“Once you melt black, you can never go back”. - ancient color maker saying.
Reply With Quote
  #37  
Old 11-04-2017, 12:06 PM
Rich Samuel's Avatar
Rich Samuel Rich Samuel is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle, WA
Posts: 2,494
Rich Samuel is on a distinguished road
"Melting red? Better off dead." - more ancient color maker saying.
Reply With Quote
  #38  
Old 11-04-2017, 01:29 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,572
Eben Horton is on a distinguished road
Quote:
Originally Posted by Rich Samuel View Post
"Melting red? Better off dead." - more ancient color maker saying.
Truth! Hahaha
Reply With Quote
  #39  
Old 11-04-2017, 07:54 PM
Marc Carmen Marc Carmen is offline
Registered User
 
Join Date: Jul 2015
Location: New Jersey
Posts: 76
Marc Carmen is on a distinguished road
Quote:
Originally Posted by David Patchen View Post
It's not just stiff, it's CRAZY stiff! Definitely the stiffest glass I've ever played with and makes the white duro feel like enamel. I gather on the new black the instant it stops moving, which is literally walking from the gh to the furnace. If you lose the core heat you're toast. If you don't transfer it directly to a stick you're toast. Gathers needs to be done before the previous one fully sets up. Pulls need to be really hot with a faster walk than usual. If you don't have the black poking out of the end of the setup and quench before you stick to the post, you're toast. It's actually super fun to work with because it's so quirky. I've not had great luck keeping it jet black--I think it might have something to do with our gh running a bit rich (maybe Pete can explain what's up w/this). It's been going graphite grey on me--I'm going a few things to try to avoid this. I've been pulling it into cane, then bundling the cane and making murrine. I haven't used the murrine yet, but it looks excellent.

If you're into twisty cane, definitely try some of this stuff, it's wild and so much fun.
Thank you David! Copied and pasted into my notes. I'm sure you saved me some headaches
Reply With Quote
  #40  
Old 11-05-2017, 08:55 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,491
Pete VanderLaan is on a distinguished road
Mark talked about cad/sel reds in fluorine that started off compatible in his work and by the time he was done, they were no longer compatible. The effects of heating and cooling repeatedly in a glass does often change them. While John is really cautious about using Hagy seals to determine mismatch, those efforts can sometimes be defeated. The description of the black makes me think of those circumstances.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #41  
Old 11-05-2017, 01:37 PM
Marc Carmen Marc Carmen is offline
Registered User
 
Join Date: Jul 2015
Location: New Jersey
Posts: 76
Marc Carmen is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
Mark talked about cad/sel reds in fluorine that started off compatible in his work and by the time he was done, they were no longer compatible. The effects of heating and cooling repeatedly in a glass does often change them. While John is really cautious about using Hagy seals to determine mismatch, those efforts can sometimes be defeated. The description of the black makes me think of those circumstances.
I've worried about this as well. Theres definitely some crystal growth going on. Some of the FeS test melts I've done needed to be struck from a dark trans brown to that characteristic gritty graphite black, but only if the melt wasn't reduced enough.

I've never had compatibility problems though. Then again, the density of the color never requires more than a thin overlay or a fine cane.
Reply With Quote
  #42  
Old 11-06-2017, 04:14 AM
David Patchen's Avatar
David Patchen David Patchen is offline
Registered User
 
Join Date: Sep 2005
Location: San Francisco, CA
Posts: 1,898
David Patchen is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
Mark talked about cad/sel reds in fluorine that started off compatible in his work and by the time he was done, they were no longer compatible. The effects of heating and cooling repeatedly in a glass does often change them. While John is really cautious about using Hagy seals to determine mismatch, those efforts can sometimes be defeated. The description of the black makes me think of those circumstances.
This is why I never use cad/sel colors in murrine. Too many heat cycles blows the fit. I got this tip from John C a decade ago.
Reply With Quote
  #43  
Old 11-06-2017, 11:26 AM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,698
Jordan Kube is on a distinguished road
Quote:
Originally Posted by Kenny Pieper View Post
I have melted that black a couple of times with no problems. Its crazy how it catches on fire when it gets charged. I stays black that's for sure!
Was the recipe similar to this one Kenny?

http://talk.craftweb.com/showthread.php?t=11375
__________________
WWUD? Think for yourself.
Reply With Quote
  #44  
Old 11-06-2017, 02:42 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,491
Pete VanderLaan is on a distinguished road
If it catches fire, it's Lino's for sure.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #45  
Old 11-07-2017, 05:49 PM
Kenny Pieper Kenny Pieper is offline
Registered User
 
Join Date: Feb 2003
Location: Burnsville N.C.
Posts: 835
Kenny Pieper is on a distinguished road
Quote:
Originally Posted by Jordan Kube View Post
Was the recipe similar to this one Kenny?

http://talk.craftweb.com/showthread.php?t=11375
Jordan I am at the Philadelphia Museum show now so I cant tell you if this is it or not. It looks about right
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 05:50 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.