Heating Refractory

My furnace is off right now due to either a loose wire, controller failure, or thermocouple problem.

Symptom: it was holding idle temp no problem (1900F). When I'd get ready to blow, I'd ramp up to 2100. At 2000, the temperature display suddenly flipped from actual to UUUU (so one of the above most likely causing it). This shut off the power to the elements until things dropped to under 2000, then it would come back on and try and recover. As I was there, I watched it happen a few times then shut it off as I was near my annual maintenance window anyway.

The most obvious suspect based on what happened is a loose thermocouple wire or connection. These things can work their way loose over time.

My plan is to tighten the connections on all the wires, and then fire up the furnace. Basically if it's a high temp (over 2000F) problem, no amount of low temp fussing will find it.

The elements have been checked and are all fine, as is power to the elements.

I want to bring the furnace up to 2100 quickly.

The crucible is out of the furnace right now as part of the overall maintenance, so the furnace is just K23, fiberfrax and alumina board.

Can I fire this up to 2000 without stopping for hours at the inversion point (900-1300F)? That is, does refractory also need to be babied through the quartz inversion or can I just crank it up? Is there a 'best ramp rate" to follow with just refractory?
Reply With Quote
  #2  
Old 10-09-2018, 03:09 PM
Scott Novota's Avatar
Scott Novota Scott Novota is offline
AbbyNormal User
 
Join Date: Jan 2004
Location: Pensacola Florida
Posts: 2,146
Scott Novota is on a distinguished road
Might also check that your controller does not have an upper limit governor on it. The last time I had this happen to me my K-type had burned up.

Last edited by Scott Novota; 10-09-2018 at 03:17 PM.
Reply With Quote
  #3  
Old 10-09-2018, 03:26 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
rEgisturd Spelunker
 
Join Date: Jan 2007
Location: USSA
Posts: 2,124
Greg Vriethoff is on a distinguished road
If nothing inside (no crucible just an empty kiln) let 'er rip. IFB and fiberfrax can take it. I assume the alumina board is outside.
__________________
I loves Dale gilhooly
Reply With Quote
  #4  
Old 10-09-2018, 04:31 PM
Rick Kellner Rick Kellner is offline
Registered User
 
Join Date: Jan 2004
Location: Hillsboro, OR
Posts: 190
Rick Kellner is on a distinguished road
I think the alumina board is the top baffle, which isolates the elements from the glass fumes.
Reply With Quote
  #5  
Old 10-09-2018, 05:51 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,487
Pete VanderLaan is on a distinguished road
solid castings should be treated with respect and go thru inversion with at least a wink and nod to expansion. Otherwise, it doesn't matter much. With the pot in, you need to behave.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #6  
Old 10-09-2018, 05:57 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,698
Jordan Kube is on a distinguished road
You should be fine. Sounds like a TC problem. Could be something lose or cracked anywhere from the thermocouple junction itself all the way back to the controller. If you are cold right now you can take the thermoucouple out of its sheath and inspect it.
__________________
WWUD? Think for yourself.
Reply With Quote
  #7  
Old 10-09-2018, 09:50 PM
Richard Huntrods's Avatar
Richard Huntrods Richard Huntrods is offline
Registered User
 
Join Date: Aug 2003
Location: Vancouver Island
Posts: 1,162
Richard Huntrods is on a distinguished road
Quote:
Originally Posted by Rick Kellner View Post
I think the alumina board is the top baffle, which isolates the elements from the glass fumes.
Correct. I could always remove it for the test.
Reply With Quote
  #8  
Old 10-09-2018, 09:52 PM
Richard Huntrods's Avatar
Richard Huntrods Richard Huntrods is offline
Registered User
 
Join Date: Aug 2003
Location: Vancouver Island
Posts: 1,162
Richard Huntrods is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
solid castings should be treated with respect and go thru inversion with at least a wink and nod to expansion. Otherwise, it doesn't matter much. With the pot in, you need to behave.
The only casting is my rammable gathering port in the maintenance lid. It's removable so I can do that for the test. I'll probably just set the lids on rather than connect up all the hinges until it's working properly.
Reply With Quote
  #9  
Old 10-09-2018, 09:58 PM
Richard Huntrods's Avatar
Richard Huntrods Richard Huntrods is offline
Registered User
 
Join Date: Aug 2003
Location: Vancouver Island
Posts: 1,162
Richard Huntrods is on a distinguished road
Quote:
Originally Posted by Jordan Kube View Post
You should be fine. Sounds like a TC problem. Could be something lose or cracked anywhere from the thermocouple junction itself all the way back to the controller. If you are cold right now you can take the thermoucouple out of its sheath and inspect it.
For sure. Loose/broken wire or loose connecting screw. I'll check the main power connections at the same time. Repeated heating/cooling cycles has been known to loosen even really tight connections.

The only odd thing is the UUUU reading (beyond upper limit). Since this controller upper limit is set to 2400F (by me) and since it was not even 2100 when it did this, it suggests either a bad connection or controller failure. I say UUUU is odd because usually broken wire will read LLLL (no signal).

Worst case I have a spare controller of another brand that I can swap in and see what happens between 2000 and 2100.
Reply With Quote
  #10  
Old 10-11-2018, 12:32 PM
Cecil McKenzie Cecil McKenzie is offline
Registered User
 
Join Date: Feb 2011
Location: Emporia, KS
Posts: 491
Cecil McKenzie is on a distinguished road
On my equipment when i have had failed thermocouples the controllers always max out and shut the whole thing down. Not sure if this is always the case.
Reply With Quote
  #11  
Old 10-18-2018, 03:59 PM
Brendan Miller Brendan Miller is offline
Registered User
 
Join Date: May 2015
Location: Rochester, NY
Posts: 6
Brendan Miller is on a distinguished road
all UUUU's usually means means thermocouple is burnt out or a leg of the thermocouple is open. Some Controllers will read LLLL or UUUU but both can be thermocouple problems.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 10:01 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.