The frost is on the pumpkin

For many years, now, as Halloween passes and the hard frosts begin, I have been worried over my glass crucibles... not the hot one filled with glass, but the retired pots decorating gardens and becoming birdbaths. Many years I have taken care to empty the water when a cold spell is upon us.

Recently, I have realized that I have never had one crack and maybe the thickness of the crucibles protect them. Have other blowers had the same experience?

Several year ago, I started insulating the surface of the water in the crucibles by floating a circle of foam wrapping (poly-ethylene?). This delays the top of the water from freezing. This is an easy solution to the potential problem, but is it needed at all?
__________________
You have to dance with the glass
Reply With Quote
  #2  
Old 11-04-2019, 08:05 AM
Eric Trulson Eric Trulson is offline
Young Turk
 
Join Date: Sep 2014
Location: Boston
Posts: 115
Eric Trulson is on a distinguished road
I'm sure they'll crack over enough freeze-thaw cycles, just like anything, but I wouldn't worry about it too much. Most pots are an inch or so of good solid stone and don't have any undercuts, so the ice layer on top can get pushed upwards by the water below freezing & expanding, instead of putting all that stress into the pot walls.

So catastrophic failure seems unlikely. The freeze/thaw cycles will just keep expanding the existing cracks in the wall until some part of the pot wall finally gives. More likely to be next decade than next year though.
Reply With Quote
  #3  
Old 11-14-2019, 01:02 PM
rodman gilder miller rodman gilder miller is offline
Registered User
 
Join Date: Aug 2014
Location: seattle
Posts: 70
rodman gilder miller is on a distinguished road
Thanks, Young Turk Eric. You are probably right that the pot thickness will win out over the ice thickness.
__________________
You have to dance with the glass
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 02:17 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.