  #76  
Old 10-22-2019, 05:59 PM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 578
Art Freas is on a distinguished road
Quote:
Originally Posted by Shawn Everette View Post
They made 4 clears, 5 if you count the cut off scraps. And I thought the two "studio" versions were compatible, one ate the hell out of your furnace, the other just had it for lunch.

96 is still coming out in some of the publication material, or is at least still on some of their distributor sites. I'm more concerned about their lack of transparency and surprise supply changes for all of their glass. I think their procurement of spectrum is going to make it even harder for the blowers, the amount of money they bank on tiles would make our appetite paltry. As you've said, no money in cullet.
Compatible and identical are different things. Assuming they are compatible in spec but not identical I wonder which side of the old the new one is.
Reply With Quote
  #77  
Old 10-23-2019, 11:02 AM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 397
Shawn Everette is on a distinguished road
I'm going to guess on the stiff side since they claim they've done away with the boric, and haven't said what else they're using for a flux.

I never tried the original "studio" nuggets, only the "new formula", which was mediocre on the blowing side, but worked fine with their sheet glass. The cut off supersaks were a mess of hot garbage. Dirty, stiff, corrosive, didn't want to fine, short pot life, and yellow. Really yellow. Though you could collect some interesting stalactites from opening of the furnace.

Last edited by Shawn Everette; 10-23-2019 at 11:25 AM.
Reply With Quote
  #78  
Old 10-23-2019, 11:07 AM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 397
Shawn Everette is on a distinguished road
I'm lucky that I can manage to buy in advance of need, so I've managed to stay ahead of the constant crisis with minimal headache.

I kinda wish bullseye was better to blow with since they seem to have their act together and might actually be able to keep with demand. Also that it was a 96. It's an odd hot glass, sloppy soup right out of the oven, then straight to a rock with no in between.
Reply With Quote
  #79  
Old 10-23-2019, 11:45 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,471
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Shawn Everette View Post
I'm going to guess on the stiff side since they claim they've done away with the boric, and haven't said what else they're using for a flux.

I never tried the original "studio" nuggets, only the "new formula", which was mediocre on the blowing side, but worked fine with their sheet glass. The cut off supersaks were a mess of hot garbage. Dirty, stiff, corrosive, didn't want to fine, short pot life, and yellow. Really yellow. Though you could collect some interesting stalactites from opening of the furnace.
****
So, what about it did you not like?
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #80  
Old 10-23-2019, 11:46 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,471
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Shawn Everette View Post
I'm lucky that I can manage to buy in advance of need, so I've managed to stay ahead of the constant crisis with minimal headache.

I kinda wish bullseye was better to blow with since they seem to have their act together and might actually be able to keep with demand. Also that it was a 96. It's an odd hot glass, sloppy soup right out of the oven, then straight to a rock with no in between.
****
And those are characteristics a caster or a fuser would want.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #81  
Old 10-23-2019, 03:33 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 397
Shawn Everette is on a distinguished road
Can't I have all the things?!
Reply With Quote
  #82  
Old 10-23-2019, 07:06 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,471
Pete VanderLaan is on a distinguished road
Not without a lot of lead.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #83  
Old 10-23-2019, 07:23 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 397
Shawn Everette is on a distinguished road
The house is pretty old, think I can get some off the walls.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 12:57 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.