SP "not food safe" disclaimer

So looking on Sp website for some annealing temps and saw the "... Not food safe, may contain lead and other chemicals." They have this disclaimer on the bottom of all their pages in a sort of general way but then it is also on their color page , bolder, which makes sense there, but does this mean no drinking glasses or bowls are to be made from their clear batch? I find it vague and confusing. Any thoughts, anybody?
Reply With Quote
  #2  
Old 02-08-2019, 09:20 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,011
Pete VanderLaan is on a distinguished road
SP contains no lead at all. It is certainly food safe but the stance from the container industry dictate that there be no lead within 1/4 inch of the lip on drinking vessels. That would include any decoration on the surface and would include any color on the cup from rod, inside or outside. There's nothing to fear from the clear and you aren't navigating legal issues.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 02-08-2019, 11:53 AM
Charles Friedman Charles Friedman is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle Wa
Posts: 569
Charles Friedman is on a distinguished road
Usually, that means "not safe for long term food storage" because of Leeching of bad stuff over time, ok for intermittent use. They did the same to the potter's glazes years ago. You can still drink from lead crystal stemware.
__________________
"Glass will save the world from ourselfs" CharlesF
Reply With Quote
  #4  
Old 02-09-2019, 07:38 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,011
Pete VanderLaan is on a distinguished road
correct, but you can't use lead crystal decanters.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 02-14-2019, 05:52 PM
Fredi Vilina Fredi Vilina is offline
Registered User
 
Join Date: Jun 2002
Location: St. Paul MN
Posts: 245
Fredi Vilina is on a distinguished road
a little clarification

Pete, so when you said no color on inside or outside within 1/4" from lip/rim does that mean color that has been encased also? Does trimming through a color that is encased now expose it partially or does it get sealed from the action of trimming?

thanks
fredi
Reply With Quote
  #6  
Old 02-15-2019, 07:26 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,011
Pete VanderLaan is on a distinguished road
I don't know. Tom Littleton had the gory details on the subject a number of years back. Perhaps it's in the archives. I recall it being more about surface decorations on the lip exterior.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 03:55 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.