Praise

I need to share how much I love the new Spruce Pine 87 formula. They found a new supplier for silica snd Lime and it has increased the optic quality of the batch considerably. I melt their ďQĒ version of 87 W/erbium and itís nothing short of water clear crystal. Itís lost if you cover in frit or use opaque bar but Iím blown away by its purity.

What I was told is that the regular SP 87 with erbium will now be as clear as the old Texas sand version which is beautiful in its own right. Before this switch I was definitely picking up tones of green in my clear work with the regular sp w/er version.

So thereís my 10Ę
__________________
<eben epoiese>
Reply With Quote
  #2  
Old 02-06-2019, 06:08 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,667
Pete VanderLaan is on a distinguished road
The "Q" is the snowflake? I knew there was an issue with grain size on the silica which was solvable. . I have loved the Minispar site for feldspar since the Kona plant burned down. I use the snowflake in my batch glasses SP mixes for me.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 02-06-2019, 07:50 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,423
Eben Horton is on a distinguished road
Q means quality. As in high quality.
Itís like looking at a piece of Steuben crystal.
__________________
<eben epoiese>
Reply With Quote
  #4  
Old 02-07-2019, 09:51 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,667
Pete VanderLaan is on a distinguished road
What is the price difference from reg SP87?
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 02-07-2019, 12:47 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,423
Eben Horton is on a distinguished road
If I remember right it was 10Ę more a pound than the 87 w/erbium. Or in other words itís the same price as the Texas sand recipe
__________________
<eben epoiese>
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 11:36 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.