  #26  
Old 08-11-2017, 12:38 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,588
Jordan Kube is on a distinguished road
Seriously though, the door system is going to lift and pivot. Think about the mechanism on a hand crank juicer with a pivot built into the neck. You lift up the handle and move the door to the side. The door itself will be 2" hard castable backed with frax just like the walls.
__________________
WWUD? Think for yourself.
Reply With Quote
  #27  
Old 08-11-2017, 03:08 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,001
Pete VanderLaan is on a distinguished road
At one point My friend Henry Summa had a track machined which was not straight. At the end it took a very orderly dive to make a door seal, so when you began to open the door, it simply began to lift away following that track. Really elegant.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #28  
Old 08-11-2017, 06:09 PM
Bill Worcester Bill Worcester is offline
Registered User
 
Join Date: Apr 2009
Location: Maui, HI
Posts: 53
Bill Worcester is on a distinguished road
Unhappy Henry

I miss Henry
Reply With Quote
  #29  
Old 08-11-2017, 07:53 PM
Cecil McKenzie Cecil McKenzie is offline
Registered User
 
Join Date: Feb 2011
Location: Emporia, KS
Posts: 472
Cecil McKenzie is on a distinguished road
Jordan .. i hope your furnace works well. i will be interested if you post your experience with it.

I have a small Denver furnace that I use sometimes in the winter so I am familiar with those elements. My furnace uses MDRs so elements may be more abused than the yours will be if you use a more advanced system of powering up your elements. i have not had much longevity with those elements and when they fail they melt severely and migrate into the refractory.

Will you use the element putty to hold the elements in place?
Some kind of mechanical method might be better.

One thing that Dennis talked about on his furnace was being able to change elements on the fly. That would be a plus because you don't have to let it cool all the way down to change elements.
Reply With Quote
  #30  
Old 08-12-2017, 08:22 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,696
Franklin Sankar is on a distinguished road
Patent application pending for Wood door on the outside as a protective device like a fuse. Over temperature can cause it to burn up like a fuse. Thanks George.

Jordan how did you clean the elements if you got any cement on them.
Franklin
Reply With Quote
  #31  
Old 08-12-2017, 08:27 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,001
Pete VanderLaan is on a distinguished road
Anybody remember those videos of the ITC coating back about fifteen years ago. They coated pieces of plywood and stuffed them up again hot furnaces? I always thought that stuff was insulating snake oil.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #32  
Old 08-12-2017, 01:45 PM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 858
Sky Campbell is on a distinguished road
ITC coatings are alive and well. Basically an advanced colloidal silica or alumina. Many people swear by it and I have seen it work on fiber pretty good. It is a bit over priced for me to buy in but it does seem to work.


Franklin a bit of brown paper to cover the element where the mortar goes. A dap of mortar then fold the paper away from element over the mortar to squish in place. When you start to heat it up you can either let the paper burn away or remove it once the water is driven from the mortar.. I used a ramable plastic for this application and recomend it over mortar. Easier to handle and will pop off clean when it's time to remove.


Jordan I like the idea and have had the same thoughts. Unfortunately I just can't justify not having a crown. The top gathering style furnace just doesn't cut it for what I want to do. I have given thoughts to the same set up with a gas fired crown on top that can be turned off at the end of the day. Not to mention could be used for reheating. I do like the idea but how are you addressing a broken pot? Where will the glass drain to? More pictures please.

I have an annealer with a lid that lifts as it turns. It is a vertical pipe with a v cut out. The door is on a smaller vertical pipe sleeved inside with a pin that sticks out. When you rotate the door the pin rides on the v cutout lifting the door as it rotates. Clear as mud? I can try and post pics of you like. It's a pretty nice trick that allows the door to sit tight on the seal until rotated.

Last edited by Sky Campbell; 08-12-2017 at 01:50 PM. Reason: It's a spelling nightmare. Where's my glasses? Why doesn't this board have a built in spell check?
Reply With Quote
  #33  
Old 08-13-2017, 02:23 AM
Steve Stadelman Steve Stadelman is offline
Registered User
 
Join Date: Jun 2002
Location: Portland oregon area
Posts: 3,731
Steve Stadelman is on a distinguished road
Sky, the problem with a gas/wire hybrid is that A1 and APM elements don't do well in reduction. You need Nichrome and it fails at several hundred degrees too low.
__________________
If all you wanted to do was express yourself artistically, you should have obtained a field watercolor set and a pad of acid-free paper. You chose a media with INFRASTRUCTURE baby!
Reply With Quote
  #34  
Old 08-13-2017, 06:14 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,696
Franklin Sankar is on a distinguished road
Sky thank you for the hint about the fold over of the brown paper The fold over trick will gEt the cement to stick better with no mess. Good one.
After working out of Michael electric furnace I could not believe how many gathering problems the crown arrangement solved.
Anyone made a crown furnace for a wire furnace? not good news about the gas wire reaction.
Franklin
Reply With Quote
  #35  
Old 08-13-2017, 03:09 PM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 858
Sky Campbell is on a distinguished road
I was thinking the elements would be isolated under a baffle. The gas fire would never see the elements. I also thought apm was proven to be not worth the money. Little gain for the money.

Yes Franklin it is commonly done. Look at a Denver furnace for reference.
Reply With Quote
  #36  
Old 08-13-2017, 03:53 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,001
Pete VanderLaan is on a distinguished road
I think APM is a genuine waste of money. I do think the French alloy would be really interesting to pursue and I don't know anyone who has done it. Street word was it was far better stuff.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #37  
Old 08-13-2017, 09:51 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,588
Jordan Kube is on a distinguished road
I like that idea for the door as well Sky.
__________________
WWUD? Think for yourself.
Reply With Quote
  #38  
Old 08-14-2017, 10:16 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,696
Franklin Sankar is on a distinguished road
Thanks Sky. I guess I will have to add the. Surface area of the crown now. More power required. It is going to be a fight.
Franklin
Reply With Quote
  #39  
Old 08-16-2017, 05:53 AM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is offline
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 661
Michael Ahlefeldt-Laurvig is on a distinguished road
John those elements are basically the same as the grill in a kitchen oven or a charcoal starter- they are just good for annealing temps- I think there are special elements rated for 1650F but I haven't used those
Reply With Quote
  #40  
Old 08-16-2017, 03:36 PM
Steve Stadelman Steve Stadelman is offline
Registered User
 
Join Date: Jun 2002
Location: Portland oregon area
Posts: 3,731
Steve Stadelman is on a distinguished road
Quote:
Originally Posted by Michael Ahlefeldt-Laurvig View Post
John those elements are basically the same as the grill in a kitchen oven or a charcoal starter- they are just good for annealing temps- I think there are special elements rated for 1650F but I haven't used those
Trust me, Jordan knows what's up.
__________________
If all you wanted to do was express yourself artistically, you should have obtained a field watercolor set and a pad of acid-free paper. You chose a media with INFRASTRUCTURE baby!
Reply With Quote
  #41  
Old 08-17-2017, 06:06 AM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is offline
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 661
Michael Ahlefeldt-Laurvig is on a distinguished road
I was answering Johns question about my annealer elements
Reply With Quote
  #42  
Old 08-17-2017, 01:54 PM
Steve Stadelman Steve Stadelman is offline
Registered User
 
Join Date: Jun 2002
Location: Portland oregon area
Posts: 3,731
Steve Stadelman is on a distinguished road
Quote:
Originally Posted by Michael Ahlefeldt-Laurvig View Post
I was answering Johns question about my annealer elements
My mistake.
__________________
If all you wanted to do was express yourself artistically, you should have obtained a field watercolor set and a pad of acid-free paper. You chose a media with INFRASTRUCTURE baby!
Reply With Quote
  #43  
Old 08-17-2017, 03:39 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,001
Pete VanderLaan is on a distinguished road
This becoming a touch esoteric. One bunch is talking about a wire melter and another is talking about annealer elements. Both are good for what they do but they're not interchangeable. Don't use stove elements in a melter unless you like strange dust. .

Ick.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #44  
Old 08-18-2017, 06:50 AM
John Riepma John Riepma is offline
Registered User
 
Join Date: Apr 2003
Location: Grand Haven, MI
Posts: 471
John Riepma is on a distinguished road
Yes, the conversation was about element coils touching and overheating and I was curious as to whether the elements that Michael had mentioned in another thread would alleviate the problem. Without knowing exactly what they were and being able to find the temp rating I thought that Micheal would be able to answer my question. I didn't mean to hijack the thread to annealers, my apologies.
Reply With Quote
  #45  
Old 08-18-2017, 08:50 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,001
Pete VanderLaan is on a distinguished road
It strikes me that one of the issues of putting elements in a moving component is how to keep the elements totally stationary as the lid moves. I did find on Amazon 10 gauge fiberglass wrapped hookup wire as well as actual 10 gauge female clips for the wire and I'm using that stuff on Mary Beth's fusing kiln which has elements in the door and the door is opened with a winch. It's working rather nicely but sourcing the heavy gauge wire had been an issue. I put it in individual sections of armored cable which makes for looking a lot like those bots in the matrix. It does keep things well isolated.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #46  
Old 09-01-2017, 01:33 PM
Dan Vanantwerp Dan Vanantwerp is offline
Registered User
 
Join Date: Apr 2017
Location: Bozeman, MT
Posts: 221
Dan Vanantwerp is on a distinguished road
Anyone know what the Denver casting mold would look like? The element groove looks like an undercut nightmare.

Some kind of a 2-part, breaks down in the middle design?
__________________
My furnace setting: 2112
Reply With Quote
  #47  
Old 09-01-2017, 02:26 PM
Rick Kellner Rick Kellner is online now
Registered User
 
Join Date: Jan 2004
Location: Hillsboro, OR
Posts: 127
Rick Kellner is on a distinguished road
Quote:
Originally Posted by Victor Chiarizia View Post
does anyone make a circular silicon carbide element that could be used instead of wire elements? vic

It's moly, but circular, anyway. How'd you like to ship that thing???
Attached Images
File Type: jpg heater-1.jpg (32.9 KB, 22 views)
Reply With Quote
  #48  
Old 09-01-2017, 02:46 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,588
Jordan Kube is on a distinguished road
Quote:
Originally Posted by Dan Vanantwerp View Post
Anyone know what the Denver casting mold would look like? The element groove looks like an undercut nightmare.

Some kind of a 2-part, breaks down in the middle design?
Screw a bunch of 2" backer rod to a sonotube. Pour it upside down so any air voids are at the top of the element grove not the bottom. That's how I did it anyway.
__________________
WWUD? Think for yourself.
Reply With Quote
  #49  
Old 09-01-2017, 03:06 PM
Dan Vanantwerp Dan Vanantwerp is offline
Registered User
 
Join Date: Apr 2017
Location: Bozeman, MT
Posts: 221
Dan Vanantwerp is on a distinguished road
Damn...that's simple! Why do I always have to complicate things?

When my kiln/furnace dies I'm thinking ahead to a larger version of what you have done here. Thanks!
__________________
My furnace setting: 2112
Reply With Quote
  #50  
Old 09-01-2017, 07:00 PM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 858
Sky Campbell is on a distinguished road
Quote:
Originally Posted by Jordan Kube View Post
Screw a bunch of 2" backer rod to a sonotube. Pour it upside down so any air voids are at the top of the element grove not the bottom. That's how I did it anyway.
Backer rod is a brilliant idea. I used rubber hose screwed to sono tube. Undid the screws removed the sono tube and then spent the day cursing and cutting tubing into little pieces till I got it out. I remember last time looking at pipe insulation but it deformed to easy. If I ever cast another that little tid bit will be a great time saver. I imagine it would be easy enough to just burn out.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 11:53 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.