Diamond bandsaw blades

I searched the archives and spent the day calling around.
I'm looking for a source for 93.5 x 1/4" blades.

The only supplier I have found for this size is Denver glass machinery. I'm sure they don't manufacture the blade themselves. I'm in the middle of a job that requires literally thousands of cuts that can only be achieved using a bandsaw. I will go thru some blades for this job and would love to find a better source with possible multi blade discounts.

Thanks for any help!
Reply With Quote
  #2  
Old 07-31-2013, 05:29 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,085
Pete VanderLaan is on a distinguished road
Did you try North Jersey Diamond?
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 07-31-2013, 10:20 PM
Patrick Casanova Patrick Casanova is offline
Registered User
 
Join Date: Apr 2002
Location: Western Wisconsin
Posts: 284
Patrick Casanova is on a distinguished road
Sky,
I have been pleased with the blades that I have gotten from these folks.

http://www.bandsawbladesdirect.com/b...and-saw-blades
Reply With Quote
  #4  
Old 08-01-2013, 10:20 AM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 1,021
Sky Campbell is on a distinguished road
Thanks

I tried jersey diamond and although they don't normally sell bandsaw blades Mark said he would look into for me. Still it would be weeks out.

Bandsaw direct only sell 1/2" I really need 1/4" for this application.
Reply With Quote
  #5  
Old 08-01-2013, 10:39 AM
George Vidas George Vidas is offline
Registered User
 
Join Date: Jun 2012
Location: Detroit, MI
Posts: 194
George Vidas is on a distinguished road
Are diamond bandsaw blades welded like normal metal/wood bandsaw blades?

Seems like the process would have to be slightly more precise to avoid having a bump or divot at the weld, since the diamond is more continuous and less textured than saw teeth.

But I wonder if there's somewhere that would sell a bunch of 1/4" diamond coil stock, and then you could take it to your local bandsaw guys and have them weld it for you.
Reply With Quote
  #6  
Old 08-01-2013, 12:23 PM
Patrick Casanova Patrick Casanova is offline
Registered User
 
Join Date: Apr 2002
Location: Western Wisconsin
Posts: 284
Patrick Casanova is on a distinguished road
Sky,
I don't know of anyone that makes a 1/4" bandsaw blade. How thick a piece do you need to cut? And how many? I believe most Ring Saws only have a 1.5" throat height, and at that thickness I think it would be really slow going.

George... "some wheels are best left round!"
Reply With Quote
  #7  
Old 08-02-2013, 06:21 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,085
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by George Vidas View Post
Are diamond bandsaw blades welded like normal metal/wood bandsaw blades?

Seems like the process would have to be slightly more precise to avoid having a bump or divot at the weld, since the diamond is more continuous and less textured than saw teeth.

But I wonder if there's somewhere that would sell a bunch of 1/4" diamond coil stock, and then you could take it to your local bandsaw guys and have them weld it for you.
***********
I would be inclined to try to remember that the goal here is to make glass with the limited time we have. It's easy to go off on tangents.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #8  
Old 08-01-2013, 02:57 PM
Tom Fuhrman Tom Fuhrman is offline
Registered User
 
Join Date: Apr 2002
Location: hills of Tennessee
Posts: 1,461
Tom Fuhrman is on a distinguished road
have you tried www.kentsupplies.com they list a 94.1" X 1/3" for $146.
Reply With Quote
  #9  
Old 08-01-2013, 05:00 PM
Hugh Jenkins Hugh Jenkins is offline
Registered User
 
Join Date: Sep 2006
Location: Honoka'a, HI
Posts: 1,007
Hugh Jenkins is on a distinguished road
www.ukam.com/diamond_band_saw_blades.htm
__________________
Aloha, Hugh
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is On
Forum Jump


All times are GMT -5. The time now is 06:39 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.