Utter Disappointment with Corning Batch Company

3 Years ago Lewis Olsen of the Corning Batch Company sold me many tons of glass that produced a "Sick Glass" effect which revealed itself as an alkaline fog that was impossible to clean off. This cost me $80,000 in returned orders from my most important client. He failed to take any responsibility for his faulty product. I have given him 3 years to at least make a gesture towards compensating my loss. I would have been happy with a couple of pallets of a different formula. But nothing, even after many promises. Feel free to let him know what a shithead he has been to me.

Last edited by Rich Arentzen; 04-10-2018 at 08:51 AM.
Reply With Quote
 


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 11:01 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.