  #26  
Old 03-29-2018, 01:46 PM
Dan Vanantwerp Dan Vanantwerp is offline
Registered User
 
Join Date: Apr 2017
Location: Bozeman, MT
Posts: 261
Dan Vanantwerp is on a distinguished road
...test your new furnace with the crucible in place.
__________________
My furnace setting: 2112
Reply With Quote
  #27  
Old 03-29-2018, 04:00 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,604
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Dan Vanantwerp View Post
...test your new furnace with the crucible in place.
******
I don't think I'd do it any other way. But I'm assuming it's not to be shut off either
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #28  
Old 03-29-2018, 05:24 PM
phil taylor phil taylor is offline
Registered User
 
Join Date: Sep 2016
Location: cincinnati, ohio
Posts: 5
phil taylor is on a distinguished road
...use sacred geometry as a way to sell furnace. i couldn't help but say it.
Reply With Quote
  #29  
Old 03-29-2018, 05:37 PM
Dan Vanantwerp Dan Vanantwerp is offline
Registered User
 
Join Date: Apr 2017
Location: Bozeman, MT
Posts: 261
Dan Vanantwerp is on a distinguished road
It can be tricky with an element melter. I was testing my first system to be sure all the connections were good...thermostat working, gauges and switches doing what they should. What I thought would take an hour took only minutes and before I knew it the temp was 300 degrees and my fresh EC pot had a hairline crack. Didn't last a whole lot longer.

I am exceedingly paranoid about my start up now but have used your crucible guide for my last couple warm-ups. Slow and steady and a good long hold at the quartz conversion point.
__________________
My furnace setting: 2112

Last edited by Dan Vanantwerp; 03-29-2018 at 06:00 PM. Reason: forgot the first pot was EC, not CC.
Reply With Quote
  #30  
Old 03-29-2018, 06:25 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,604
Pete VanderLaan is on a distinguished road
AH, well, that makes sense. It's OK to put all your eggs in one basket, BUT WATCH THAT BASKET! EC makes a perfectly reasonable pot. I designed most of the round bottom ones they have and they have a reasonable mix, but sort of sloppy. I don't know what a "CC" pot is. Best to splurge on a controller. In Electric it's really easy to manage.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #31  
Old 03-29-2018, 06:27 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,604
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by phil taylor View Post
...use sacred geometry as a way to sell furnace. i couldn't help but say it.
******
In Texas they used to say "Diamonds as big as horse turds..."
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #32  
Old 03-29-2018, 06:31 PM
phil taylor phil taylor is offline
Registered User
 
Join Date: Sep 2016
Location: cincinnati, ohio
Posts: 5
phil taylor is on a distinguished road
beautiful! I will to use that.
Reply With Quote
  #33  
Old 03-29-2018, 06:52 PM
Dan Vanantwerp Dan Vanantwerp is offline
Registered User
 
Join Date: Apr 2017
Location: Bozeman, MT
Posts: 261
Dan Vanantwerp is on a distinguished road
Crucible Connection=CC

Your "CC" 80 lbers are 1" thick...that EC one was maybe 1/2". I find them much more resistant to thermal shock.
__________________
My furnace setting: 2112
Reply With Quote
  #34  
Old 03-29-2018, 07:12 PM
Dan Vanantwerp Dan Vanantwerp is offline
Registered User
 
Join Date: Apr 2017
Location: Bozeman, MT
Posts: 261
Dan Vanantwerp is on a distinguished road
I also recall that I went with a straight walled version of the 80 lb EC...5/8" thick actually. I should have gone with the round bottom version

That was awhile ago. I didn't mean to denigrate EC...just pointing out a moment I wish I could take back.
__________________
My furnace setting: 2112
Reply With Quote
  #35  
Old 03-29-2018, 08:32 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,604
Pete VanderLaan is on a distinguished road
I only did the round bottomed ones. The two 80 lb pots are the same mold.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 05:14 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.