brief explanation of the two couples thread
Brian recently posted a thread about a failed melt and his question revolved around his dual thermocouples. It was not the case that they were the problem. Lots of things can go wrong with a melt. It is being looked at. Brian decided on his own to delete the thread , given that the potentials for speculative error were simply going to do no good and resolve nothing.
The question is now with the people who test such things. I think it's being handled well. Just in case you had questions.
__________________
Where are we going and why am I in this basket? |
#2
|
||||
|
||||
Thanks Pete. I'm sure I'm not the only one paying attention.
|
#3
|
||||
|
||||
Thanks for posting this Pete. I was hesitant to delete but wanted to err on the side of caution.