CraftWEB Hot Glass Talk  

Go Back   CraftWEB Hot Glass Talk > Hot Glass > General Hot Glass Discussion

Reply
 
Thread Tools Display Modes
  #1  
Old 05-30-2012, 08:42 PM
Josh Bernbaum Josh Bernbaum is offline
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 724
Josh Bernbaum is on a distinguished road
Yellow Iron oxide?

Anyone tried using yellow iron oxide instead of the red iron oxide?
Hoping to throw some in with my next transparent color melt, but wondering
if I should be expecting a similar green that the red iron oxide makes or not.
Thanks.
Reply With Quote
  #2  
Old 05-30-2012, 09:23 PM
Dave Bross Dave Bross is offline
Registered User
 
Join Date: Apr 2002
Location: Archer FL(near Gainesville)
Posts: 2,953
Dave Bross is on a distinguished road
If it's a different color iron I would expect it to have a different level of oxidation/reduction.

Iron is sensitive to oxygen levels so you can probably expect a different color.

Maybe not different enough to even notice though.
__________________
Art is not a thing...it's a way.
Reply With Quote
  #3  
Old 05-31-2012, 05:50 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,274
Pete VanderLaan is on a distinguished road
It will really be a question of valence and oxygen supplied. Iron can have a lot of different valences. FeO, Fe203, Fe305... on and on.I have actually never heard of "Yellow" iron. Red and Black, Yes, Yellow, no. Some glasses want a lot of 02, some don't. It depends on your needs.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 05-31-2012, 07:16 PM
Josh Bernbaum Josh Bernbaum is offline
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 724
Josh Bernbaum is on a distinguished road
Did a melt today.
224g yellow iron oxide and 114g red copper oxide mixed in 50# SP87.
This recipe was courtesy of Ed Branson in western Massachusetts, although his had red iron and black copper.
Seems to be a nice turquoise-green.
The one at the top was my previous melt with a tiny bit of cobalt for the light blue.
Attached Images
File Type: jpg photo.JPG (35.1 KB, 62 views)
Reply With Quote
  #5  
Old 05-31-2012, 08:08 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,274
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Josh Bernbaum View Post
Did a melt today.
224g yellow iron oxide and 114g red copper oxide mixed in 50# SP87.
This recipe was courtesy of Ed Branson in western Massachusetts, although his had red iron and black copper.
Seems to be a nice turquoise-green.
The one at the top was my previous melt with a tiny bit of cobalt for the light blue.
******************
The top one actually looks like an intense copper glass to me Josh and the bottom certainly looks like iron and copper. Good Job!
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #6  
Old 05-31-2012, 11:17 PM
Jon Myers's Avatar
Jon Myers Jon Myers is offline
Registered User
 
Join Date: Apr 2002
Location: Portland OR
Posts: 631
Jon Myers is on a distinguished road
yellow Iron oxide is common enough in ceramics. I think it is less intense than red and black but I don't really remember... Its used in crystalline glazes
Reply With Quote
  #7  
Old 06-01-2012, 09:36 AM
Steven O'Day Steven O'Day is offline
Registered User
 
Join Date: Jun 2002
Location: portland oregon
Posts: 339
Steven O'Day is on a distinguished road
Yellow iron - Fe2H2O4
Black iron Fe3O4
Red iron – Fe2O3
Reply With Quote
  #8  
Old 06-01-2012, 09:54 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,274
Pete VanderLaan is on a distinguished road
Here's more: ( Thanks Steve.)

Here's what that trustworthy wikipedia says: ( Wanna buy a bridge?)
The monohydrate (FeO(OH)·H2O) might otherwise be described as iron(III) hydroxide (Fe(OH)3), and is also known as hydrated iron oxide or yellow iron oxide.

You're buying contaminated water Josh.
Also:

What is important about it is that iron becomes a nucleation point for the growth of crystals which is why many old copper ruby formulas call for Iron in the mix.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 02:56 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.