spodumene

I am thinking of changing my recipe since Lithium Carb. is now $14.95 a lb.I have access to 1000 lb of spodumene . It does not show the Fraction or reciprocal in Glass Notes, does anyone know where I can find the info to sub spodumene for 1.25 lbs of Litium Carb.
Reply With Quote
  #2  
Old 07-25-2017, 12:35 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,716
Pete VanderLaan is on a distinguished road
Spodumene is a typical feldspar. If you go the pages in glassnotes which give out the percents, just plug in lithium where it indicates either sodium or potassium. Something like 13-14%. John Croucher did have me using a 4.90 expansion coefficient for the lithium. As is often the case, the downside is tramp iron in your formula.

You need to account for the silica and the alumina in the spar. Without looking it up, it seems to me the silica is about 67% and the alumina 17%
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 07:01 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.