Hello All,

I'm thinking I'll start to dip my toes into the world of lead glasses. I have no idea where to start, I've usually steered away from lead for health reasons. But since I've started using selenium in my gold ruby (amazing results by the way, thank you Pete), I figure my self preservation has gone out the window. I'd imagine the best place to start for this would be a clear lead base. From there, could it be used with (hopefully) minimal modification to accommodate gold?
Reply With Quote
  #2  
Old 07-11-2019, 12:12 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,310
Pete VanderLaan is on a distinguished road
Gold colors always do best in a lead base. Always add a tiny amount of selenium to those melts. The hard part is getting the lead. These days, I see the bisilicate sold for $20 dollars a lb. I pay 98 cents for it in Shanghai. I can't import it. At this point here, I have about 350lbs of the monosilicate and the litharge left maybe a bit more and that will take me to the end of the line. I rarely melt it anymore.

Your health will be fine. Ventilate the facility well. wear gloves and a respirator. Jordan's little grow booth would work well.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 07-11-2019, 07:42 PM
Josh Bernbaum Josh Bernbaum is offline
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 733
Josh Bernbaum is on a distinguished road
I've heard melts with Pb do better in clay pots versus our typical alumina ones.
Any truth to this?
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #4  
Old 07-12-2019, 07:12 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,310
Pete VanderLaan is on a distinguished road
Clay is ideal but I've done lead melts in the High Temp alumina pots for years and it's fine. I doubt you would notice a difference in a smaller pot. What's important is controlling the atmosphere.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 04:49 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.