Watlow EZ

Greetings,
My Watlow 981 on my annealehr finally bit the dust. I replaced it with the Watlow EZ. I am learning a bit on programming but it is not sure intuitive. Has anyone programmed an annealing cycle with one of these? Can you walk through the steps involved?
Thanks,
Andy
__________________
Keep It Centered
http://aboatman.blogspot.com
http://bluesagestudios.blogspot.com
Reply With Quote
  #2  
Old 07-14-2017, 12:45 PM
Steve Stadelman Steve Stadelman is offline
Registered User
 
Join Date: Jun 2002
Location: Portland oregon area
Posts: 3,728
Steve Stadelman is on a distinguished road
Send it back for a refund and buy a SOLO control for $90.00 from automation direct. It will be intuitive to program with an easily read guide and phone help.
__________________
If all you wanted to do was express yourself artistically, you should have obtained a field watercolor set and a pad of acid-free paper. You chose a media with INFRASTRUCTURE baby!
Reply With Quote
  #3  
Old 07-16-2017, 02:02 AM
Dennis Hetland Dennis Hetland is offline
Registered User
 
Join Date: Sep 2009
Location: Salem, OR
Posts: 304
Dennis Hetland is an unknown quantity at this point
Quote:
Originally Posted by Andrew Boatman View Post
Greetings,
My Watlow 981 on my annealehr finally bit the dust. I replaced it with the Watlow EZ. I am learning a bit on programming but it is not sure intuitive. Has anyone programmed an annealing cycle with one of these? Can you walk through the steps involved?
Thanks,
Andy
IF You get the USB Port attachment all you have to do is plug your laptop into it, fill out the graph and it's programmed. Very quick and easy.
You can add a usb port to most of the cheap $!00 one as well.
__________________
candlewoodglass@gmail.com
Reply With Quote
  #4  
Old 07-16-2017, 10:08 PM
Daniel Sviland Daniel Sviland is offline
Registered User
 
Join Date: Apr 2012
Location: Waukegan, IL
Posts: 15
Daniel Sviland is on a distinguished road
I did the same about a year ago, I called Watlow and their tech walked me thru doing the programming step by step for 30 minutes plus on the phone.
Worked flawlessly so far.
Dan
Reply With Quote
  #5  
Old 07-17-2017, 07:37 AM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is online now
(((0)))
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 1,898
Greg Vriethoff is on a distinguished road
Watlow does have good customer support.
__________________
"It's such a fine line between stupid and clever." - David St. Hubbins
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 08:46 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.