#1
|
||||
|
||||
96 glass color from China on eBay
Several colors in small diameter rod for sale as "unbranded". Seller is idea*for*life
Anyone ever try this material?
__________________
"It appears to me that glass men are the most given to drunkeness of any class of men I know" Peter Burt, recruiter in Europe, in a letter to Deming Jarves of the Boston and Sandwich glass company. -1826 |
#2
|
||||
|
||||
well, better detail would help Ted. I know a number of the color makers in the PRC but the issue is still whether there is engineering to maintain the quality control. In the Shanghai shop , it exists but that's not saying much when you look over the industry. We're not selling color, we use it.
__________________
Where are we going and why am I in this basket? |
#3
|
||||
|
||||
Well I had thought that providing the sellers name would make finding one of the sale items easy to find. As I now see that this seller has 419 listings on eBay, that was a poor assumption. Here is one of the colors in question.
https://m.ebay.com/itm/1kg-2-2-lb-Fu...sAAOSw7ThUfxCy There is not much information in the listing but maybe someone here will spot something I missed.
__________________
"It appears to me that glass men are the most given to drunkeness of any class of men I know" Peter Burt, recruiter in Europe, in a letter to Deming Jarves of the Boston and Sandwich glass company. -1826 |
#4
|
|||
|
|||
Doesn't seem like you'd be saving much compared to what East Bay or Olympic can offer, and at least you know what you're getting with them.
|
#5
|
|||
|
|||
PI glass......hmmmmmm who had that name?
|
#6
|
||||
|
||||
I agree with Mike on the price and it also seems to me to be an odd shape to make a 96 in. I could see it as a 104 or a boro certainly. I'll ask Eveline. That takes time now since the PRC doesn't allow email from the west in Shanghai. She has to have a VPN in Hong Kong.
__________________
Where are we going and why am I in this basket? |
#7
|
||||
|
||||
*****
You're right James. Wasn't that the off shot from Seattle Batch at one point ten years back or was it someone else?
__________________
Where are we going and why am I in this basket? |
#8
|
|||
|
|||
that looks like 10 year old color to me
|
#9
|
|||
|
|||
I noticed it said Spectrum in the description.
__________________
<eben epoiese> |
#10
|
||||
|
||||
********
Moomka visits the far east?
__________________
Where are we going and why am I in this basket? |
#11
|
|||
|
|||
That is old stock from PI, whoever made it ended up with a lot of stock....
I wonder when they will push old china nuggets back on the market. |
#12
|
||||
|
||||
It makes much more sense. It's certainly pricey