#1
|
||||
|
||||
Repairing wire elements
The hole I drilled to pass my thermocouple into the furnace was too close to the element. The element is above the thermocouple tube and is resting on the tube now. I suspect it will continue to droop and who knows where it will drop/roll/move to.
I will try to get a pic but in the meantime, any idea on how to repair? Anyone joined brittle elements? how? The element is resting loosely on the tube , I was thinking about how to pin it from falling further down. Franklin |
Thread Tools | |
Display Modes | |
|
|