Repairing wire elements

The hole I drilled to pass my thermocouple into the furnace was too close to the element. The element is above the thermocouple tube and is resting on the tube now. I suspect it will continue to droop and who knows where it will drop/roll/move to.
I will try to get a pic but in the meantime, any idea on how to repair? Anyone joined brittle elements? how?
The element is resting loosely on the tube , I was thinking about how to pin it from falling further down.
Franklin
Reply With Quote
  #2  
Old 12-03-2009, 02:46 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,660
Pete VanderLaan is on a distinguished road
Joining a brittle element is easy Franklin. Heat the ends with a torch until it glows and gently pull the wire straight. Just be easy. It will straighten right out. Do it to both ends, and when you want to twist them together just make sure the wire is glowing when you manipulate them in any way. Then, pin them and pin them deep.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 12-03-2009, 05:52 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,755
Franklin Sankar is on a distinguished road
Thanks Pete. This is one job that I never anticipated was possible. Maybe because of the small cavity I have to work in. The pics does not make it easier because they fool you. I realized that a picture is a useful tool is examining the inside of the furnace. I am able to see it from a different angle and am able to see some parts that were not possible from outside. The elements are resting on a grove but it looks like its on the edge.
Now that you can see it. How about if I heat it and cut it then pull them together and twist. Or just heat the excess and twist it?
Franklin
Attached Images
File Type: jpg element2.jpg (43.4 KB, 84 views)
File Type: jpg element 1.jpg (44.9 KB, 81 views)

Last edited by Franklin Sankar; 12-03-2009 at 05:58 PM.
Reply With Quote
  #4  
Old 12-03-2009, 06:37 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,660
Pete VanderLaan is on a distinguished road
Cutting the wire is easier when hot than cold. Cold, it's really brittle. If someone can help you, have them heat the wire while you hold both ends with needlenose pliers. Holding both ends is important so you don't stress the unheated part of the wire cuz if you do, it will break and then you will have to fix that too. Holding one end, that part in the groove, heat the portion you wish to pull away and just do it gently and it will come. Make it fairly straight. Then do the other section. With both hot, twist them together. It's really easy once you figure it out. While it's hot, try to make the wire stay in a straight line so it will be easier to re-install.

I did my entire annealer with old element scraps back in the summer. I just didn't have the money for new ones. I had literally twenty pieces of wire all broken up. I heated and connected every one of them, made three separate complete elements and they are all working just fine. I have just been reconnecting this stuff for years. I have a big box of element scrap.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 12-03-2009, 06:58 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,755
Franklin Sankar is on a distinguished road
Thanks Pete and you get the WWDD award for 2009.
Work hotter work hotter. Than damn man shouting it to me again. I will never forget that.
Franklin
Reply With Quote
  #6  
Old 12-03-2009, 07:37 PM
Marcel Braun Marcel Braun is offline
Registered User
 
Join Date: Sep 2005
Location: Oregon
Posts: 126
Marcel Braun is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
Joining a brittle element is easy Franklin. Heat the ends with a torch until it glows and gently pull the wire straight. Just be easy. It will straighten right out. Do it to both ends, and when you want to twist them together just make sure the wire is glowing when you manipulate them in any way. Then, pin them and pin them deep.
Once again I am glad I take the time to read this forum.

THX.
Reply With Quote
  #7  
Old 12-03-2009, 10:02 PM
R. Scott Johnson R. Scott Johnson is offline
Registered User
 
Join Date: Oct 2004
Posts: 460
R. Scott Johnson is an unknown quantity at this point
this really is great information. never would have thought of such repairs.
thanks again!
do moly elements get repaired the same way?
Reply With Quote
  #8  
Old 12-04-2009, 12:55 AM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,650
Jordan Kube is on a distinguished road
Unfortunately no. Sure would be nice if you could put them back together.
__________________
WWUD? Think for yourself.
Reply With Quote
  #9  
Old 12-04-2009, 06:27 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,660
Pete VanderLaan is on a distinguished road
Just finding all of the parts of the moly element is damn near impossible. Moly elements are like a bent wheel. It can't be mended.

I'm not sure how long the fix is in a wire melter. If it breaks from natural causes, I would replace it but in a spot like Franklin's I think it's worth the effort. Keep the mend area as short as you possibly can. In an annealer they will last for a long long time. Remember to pin it. It's not coiled anymore so it will sag a lot. I think the last time I had to buy an element was about fifteen years ago. Pinning is usually done using the same material if you have some short new sections, or straighten out some old stuff and use it. On annealers, I use 2 1/2 inch stainless screws and those last forever.

Maybe this is one of those dumb short threads that belongs in antiques and classics.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #10  
Old 12-04-2009, 11:41 AM
Dave Bross Dave Bross is offline
Registered User
 
Join Date: Apr 2002
Location: Archer FL(near Gainesville)
Posts: 2,949
Dave Bross is on a distinguished road
I vote for "antique and classic-ing" this one.

Anything that makes me feel bad all over again about a lot of stuff I've tossed, like damn near new elements with one "indescretion" (read as fumble glass on one spot), is a classic.

Maybe put something in the title about repairing elements?
__________________
Art is not a thing...it's a way.

Last edited by Dave Bross; 12-04-2009 at 11:46 AM.
Reply With Quote
  #11  
Old 12-04-2009, 11:48 AM
Scott Novota's Avatar
Scott Novota Scott Novota is online now
AbbyNormal User
 
Join Date: Jan 2004
Location: Pensacola Florida
Posts: 2,130
Scott Novota is on a distinguished road
crap!

I wish I had read this about 2 weeks ago. Looking at what was done and how to repair it I could have fixed it easy.


Next time Gadget....next time.....



Scott.
.
Reply With Quote
  #12  
Old 12-04-2009, 12:08 PM
Lawrence Ruskin Lawrence Ruskin is offline
Registered User
 
Join Date: Sep 2006
Location: Lions Bay B.C.
Posts: 706
Lawrence Ruskin is on a distinguished road
It was mentioned a while back.

Having somewhere on the net the accumulated wisdom on just repairing and comparing wire melter is a good idea.

Prices for ''off the shelf'' units, durability, capacity and how much they cost to run, and information on building your own.

Competition drives innovation.

A sticky on this site for example.

You could of course do one for any type of melter....
Reply With Quote
  #13  
Old 12-04-2009, 01:29 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,660
Pete VanderLaan is on a distinguished road
I will try to do something. I had no idea that this was not fairly common knowledge.There is a lot of garbage in my head after forty five years of this stuff. I really don't know how well it will work on a melter. Annealers yes.

Changing the title of a thread is actually impossible. I might be able to merge it into a thread of a different name. "Suspending Elements" isn't half bad. It makes me think about High School and how easy it was to get in trouble.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #14  
Old 12-04-2009, 01:38 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,660
Pete VanderLaan is on a distinguished road
Well, that was wrong. Changing the name was really easy.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is On
Forum Jump


All times are GMT -5. The time now is 12:15 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.