I have a customer that wants to put some glass outside next to the pool. I think itís kind of crazy and advised against it but I know people do it.

I had a piece in my carport the other day for only 30 minutes, it got so hot I could hardly touch it. I just donít see how that is good for the glass.

What is your experience?
How about candles in glass?
Reply With Quote
  #2  
Old 10-12-2018, 01:20 PM
James Ennis James Ennis is offline
Registered User
 
Join Date: Oct 2004
Location: seattle
Posts: 328
James Ennis is on a distinguished road
someone just told me the pool chemicals had etched the glass art they had hung
above the pool.
Reply With Quote
  #3  
Old 10-12-2018, 02:00 PM
Ed Pennebaker's Avatar
Ed Pennebaker Ed Pennebaker is offline
Registered User
 
Join Date: Apr 2002
Location: Red Fern Glass near Green Forest, AR
Posts: 204
Ed Pennebaker is on a distinguished road
I have some cast glass pieces that have been outside for years and are looking fine. Some are SP87, some Gabbert Cullet, some cullet from the old Southwestern Glass factory in Ft. Smith, AR. Also have some blown pieces from the same glass that have been outdoors. The ones that have broken usually have taken direct hits from falling hickory nuts.
Reply With Quote
  #4  
Old 10-12-2018, 04:28 PM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 977
Sky Campbell is on a distinguished road
Well if there is a problem I have a few thousand pieces I need to recall.. Obviously you don't want something that can hold water and freeze or act like a magnifying glass and set the yard a fire. I have yet to experience a problem and I do a lot of outdoor installations. The pool etching sounds plausible but I would think you would see it on windows surrounding inside pools.
Reply With Quote
  #5  
Old 10-12-2018, 07:28 PM
Barb Sanderson's Avatar
Barb Sanderson Barb Sanderson is offline
Registered User
 
Join Date: Apr 2002
Location: rainy, foggy, chilly northwest seattle
Posts: 1,096
Barb Sanderson is on a distinguished road
As some of you know, I made glass art for gardens for 15 years. As Sky mentioned .... you can leave glass outside year round as long as it doesn't hold water and freeze and expand = cracks
Also you don't want to put glass outside in the sun in a warm climate and right next to a sprinkler system - thermal shock could happen.
But after 15 years working with glass in gardens my experience with breakage is most common where tree limbs fall onto the glass. Hope this helps.
?Barb
Attached Images
File Type: jpg spears2lg.jpg (88.9 KB, 40 views)
Reply With Quote
  #6  
Old 10-13-2018, 12:22 AM
Rich Samuel's Avatar
Rich Samuel Rich Samuel is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle, WA
Posts: 2,507
Rich Samuel is on a distinguished road
A friend swears he lost a homemade "Chihuly Javelin" (his term) one sub-freezing morning when his dog peed on it.
Reply With Quote
  #7  
Old 10-13-2018, 03:21 AM
Chris Lowry Chris Lowry is offline
Registered User
 
Join Date: Oct 2003
Posts: 274
Chris Lowry is on a distinguished road
Iíve always errored on the side of caution but I guess it works. Thanks for the input.
Reply With Quote
  #8  
Old 10-13-2018, 10:25 AM
Tom Fuhrman Tom Fuhrman is offline
Registered User
 
Join Date: Apr 2002
Location: hills of Tennessee
Posts: 1,441
Tom Fuhrman is on a distinguished road
I have a lot of sculptures that have been outside for 20 years and have had no problems. I have a lot in my own yard and displayed in my gardens and deck. Like everyone said, freezing water within a trapped area is outdoor glass's enemy.
Reply With Quote
  #9  
Old 10-13-2018, 10:54 AM
David Hopman David Hopman is offline
Registered User
 
Join Date: Mar 2009
Location: Sutter Creek, CA
Posts: 440
David Hopman is on a distinguished road
I hung a string of cracked 9" colored floats in a tree 18 years ago in front of the shop and they are still there.
Reply With Quote
  #10  
Old 10-13-2018, 06:53 PM
Tom Fuhrman Tom Fuhrman is offline
Registered User
 
Join Date: Apr 2002
Location: hills of Tennessee
Posts: 1,441
Tom Fuhrman is on a distinguished road
they have been using glass floats on fishing nets for many, many, years.
Reply With Quote
  #11  
Old 10-15-2018, 07:18 AM
Monte G Becker Monte G Becker is offline
Registered User
 
Join Date: Feb 2018
Location: Hadley Massachussets
Posts: 14
Monte G Becker is on a distinguished road
Garden Dangers

Early on, pieces would occasionally get away from me. They'd be a couple of feet long with a thing stem and a thicker bulb. "Ahhh - yeah, that was intentional..." I'd say. "Good as a garden ornament..."

Friends indulged me and took these pieces for their garden. Then, got the call that the fire department arrived. Dry mulch, hot sun and the magic of magnification...

On the other hand, that's the only pieces I've ever lost to the elements!
Reply With Quote
  #12  
Old 10-17-2018, 02:56 PM
Scott Novota's Avatar
Scott Novota Scott Novota is offline
AbbyNormal User
 
Join Date: Jan 2004
Location: Pensacola Florida
Posts: 2,150
Scott Novota is on a distinguished road
I have a piece have lived though all of this outside:

#1. Hurricane Ivan, Hurricane Opal, Hurricane Denis, and now Hurricane Michael.

#2. Hail, light dusting of what some would call snow I called frost, massive amounts of rain and blistering direct heat from direct sunlight.

#3. Weed Wacker...many years worth of "woah forgot that was there!"

#4. Being picked up at the start of a Mardi Gras Parade as the "Scepter of the Admiral" of a float. It made it though a full day of parading, drinking until 3 am, and placed back in it's original location.

#5. Used as a putter to demonstrate his neighbors 70 foot putt at Augusta National with golf ball strike for effect.

I need to go pull that yard spike, it is pretty big actually, and re-secure the pole that is attaching it to the ground. It is however quite hardy and lived a full life of adventure. We have named it but I am pretty sure it is something that would get me sent to sensitivity training now days.

Last edited by Scott Novota; 10-17-2018 at 02:58 PM.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 05:46 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.