CraftWEB Hot Glass Talk  

Go Back   CraftWEB Hot Glass Talk > Hot Glass > General Hot Glass Discussion

Reply
 
Thread Tools Display Modes
  #1  
Old 07-17-2020, 07:31 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,078
Franklin Sankar is on a distinguished road
Scale in cullet

If you have bits of scale in the cullet for remelting. Does it drill holes in the pot, or affect the small pot.
Franklin
Reply With Quote
  #2  
Old 07-18-2020, 06:05 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,078
Franklin Sankar is on a distinguished road
Ok I do it to practice sometimes.
Franklin
Reply With Quote
  #3  
Old 07-18-2020, 08:49 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,707
Pete VanderLaan is on a distinguished road
If your work is entirely clear, yes the iron tone will show. If you are adding color, you'll likely never see it at all.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 07-18-2020, 09:54 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,078
Franklin Sankar is on a distinguished road
So it does not harm the pot. Donít care about coloring .
Franklin
Reply With Quote
  #5  
Old 07-18-2020, 11:50 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,707
Pete VanderLaan is on a distinguished road
It does not harm the pot.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #6  
Old 07-18-2020, 12:03 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,078
Franklin Sankar is on a distinguished road
Great. Thanks
Franklin
Reply With Quote
  #7  
Old 07-18-2020, 08:02 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,863
Eben Horton is on a distinguished road
Add a wee bit of iron oxide to it and enjoy some Black Forest glass. It is so beautiful.
__________________
<EBEN EΠOIESEN >
Reply With Quote
  #8  
Old 07-19-2020, 06:11 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,078
Franklin Sankar is on a distinguished road
Is it easy to clean the pot after. I can’t get all the glass out.
Franklin
Reply With Quote
  #9  
Old 07-19-2020, 12:57 PM
Hugh Jenkins Hugh Jenkins is offline
Registered User
 
Join Date: Sep 2006
Location: Honoka'a, HI
Posts: 1,044
Hugh Jenkins is on a distinguished road
It can take a charge to wash out the tint, but it really depends on how clean the batch is that you are charging. As long as you don't scrupulously sort your cullet you will keep recycling the iron (and chrome) from pipe scale. We save out the "near clear" and wait for a time close to crucible replacement and plan for some tinted melts. At least the scale dissolves in well.
__________________
Aloha, Hugh
Reply With Quote
  #10  
Old 07-20-2020, 10:14 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,078
Franklin Sankar is on a distinguished road
Thanks I was worried that the scale would drill holes in the pot.
All is well now
Franklin
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 08:07 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.